1-20 of 25 Search Results for

Colmonoy no. 6

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1963) 12 (1): Ni-78.
Published: 01 January 1963
... Colmonoy No. 6 is a high-carbon, nickel-base alloy recommended for hard facing parts to resist wear, corrosion, heat and galling. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1974) 23 (6): Ni-205.
Published: 01 June 1974
... *Special specimens having l/2-inch-radius notch and polished to remove all possibility of stress concen- trations. Table 3 - TYPICAL WHEELS FOR GRINDING COLMONOY NO. 62SA (Deposits produced by spraying powder and fusing) 0.28 1 7.80 1875 0.109 8.1 x 10-6 104 0.10 1.005 32 x 106 Make Surface of Horizontal...
Journal Articles
Alloy Digest (1974) 23 (7): Ni-206.
Published: 01 July 1974
... COLMONOY No. 69 is a nickel-base hard-surfacing alloy incorporating the attractive qualities of Colmony No. 6 plus greatly improved out-of-position fusing characteristics. Its extended plastic range means that sagging and running of other-than-horizontal surfaces during finishing is virtually...
Journal Articles
Alloy Digest (1964) 13 (1): Co-36.
Published: 01 January 1964
... Wallex No. 6 is a cobalt-base alloy recommended for hard facing parts to resist impact, corrosion and oxidation at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture...
Journal Articles
Alloy Digest (1976) 25 (7): Ni-230.
Published: 01 July 1976
.... Workability: Deposits of Colmonoy No. 8 cannot be hot or cold worked. This is true even in the plastic range (1740-19750F). Corrosion and Abrasion Resistance: Colmonoy No. 8 contains approximately two times as much chromium as Colmonoy No. 6. Most of this chromium is in solid solution; therefore. No. 8 has...
Journal Articles
Alloy Digest (1977) 26 (3): Ni-242.
Published: 01 March 1977
... Deposits 28-33 Class 6* Class 2* Class 1* Class 5 * Class 3 * Class 3 * Investment Castines 28-33 Class 6* Class 2* Class 1* Class 5 * Class 3* Class 3 * *Classified on a comparative basis of 1 (highest) to 6 (lowest). Table 2 - TYPICAL WHEELS FOR GRINDING COLMONOY No. 22 (Fuseweld and welding rod deposits...
Journal Articles
Alloy Digest (1977) 26 (1): Ni-239.
Published: 01 January 1977
... resistance Class 5 * Red hardness Class 3* Weldability Colmonov No 3 4 .- . Class 3* Colmonoy No. 24 Class 4* *Classified on a comparative scale of 1 (highest) to 6 (Icwest). Table 2 - TYPlCAL WHEELS FOR GRINDING COLMONOY No. 23A AND No. 24 (Fuseweld deposits) Make Surface 0.310 8.60 1950 1790 of Horizontal...
Journal Articles
Alloy Digest (1974) 23 (10): Ni-210.
Published: 01 October 1974
... COLMONOY No. 70 and No. 72 contain high tungsten which hardens the matrix and provides superior hard-facing materials. No. 70 hasexcellent resistance to fretting corrosion. No. 72 is harder than No. 70 and provides better resistance to low-stress abrasion and is well suited to resist scouring...
Journal Articles
Alloy Digest (1975) 24 (6): Ni-218.
Published: 01 June 1975
... COLMONOY NO. 52SA comprises a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat and galling. Deposits, which have only moderate hardness (Rockwell C 45-50), may be machined with carbide tooling. Also, deposits have fairly good ductility and impact strength...
Journal Articles
Alloy Digest (1976) 25 (5): Ni-227.
Published: 01 May 1976
... COLMONOY No. 42SA is a nickel-base alloy recommended for hard surfacing parts to resist wear, heat, corrosion and galling. Deposits have a moderate hardness of Rockwell C 35-40 and can be machined with carbide tooling. Also, deposits have fairly good workability, ductility and impact strength...
Journal Articles
Alloy Digest (1977) 26 (6): Ni-245.
Published: 01 June 1977
... (1051) 0.107 9.1 x 10-6 104 0.10 1.005 32 x 106 Heat Treatment: Colmonoy No. 56 cannot be hardened or strengthened by additional heat treatment. Machining, Grinding and Lapping: Colmonoy No. 56 can be machined readily with carbide-tipped tools such as Kennametal K6, Carboloy 883, or equivalent...
Journal Articles
Alloy Digest (1975) 24 (5): Ni-217.
Published: 01 May 1975
... COLMONOY NO. 5 comprises a chromium-boride-containing, nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat and galling. Deposits, which have only moderate hardness (Rockwell C 45-50), may be machined with carbide tooling. Also, deposits have fairly good...
Journal Articles
Alloy Digest (2008) 57 (9): Ni-665.
Published: 01 September 2008
... Colmonoy No. 63HV is a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat, and galling. The hardness of Colmonoy 63HV ranges to 58–61 HRC, and it is resistant to abrasion. Colmonoy 63HV is sized exclusively for high-velocity oxygen-fuel thermal spray systems...
Journal Articles
Alloy Digest (1995) 44 (9): Ni-486.
Published: 01 September 1995
... COLMONOY No. 68 is specifically designed for centrifugal casting of bimetallic barrels and liners for corrosive applications such as fluoropolymer processing. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1998) 47 (9): Ni-545.
Published: 01 September 1998
... but somewhat less than Colmonoy alloys 86 and 6 (See Al/w Digest Ni-227 and Co- 36 See Fip. 3. General Characteristics: Colmonoy 98 is a patented nickel-base hard-surfacing alloy with su- perior resistance to corrosive liquids. It has a low coefficient of fric- tion to reduce metal-to-metal adhesive wear loss...
Journal Articles
Alloy Digest (1998) 47 (10): Ni-546.
Published: 01 October 1998
... Colmonoy 750 is a tough Ni-Cr-W matrix alloy used to hold extremely hard tungsten-carbide particles. It is best used for the most severe abrasive conditions and is finished by grinding. This datasheet provides information on composition, physical properties, microstructure, hardness...
Journal Articles
Alloy Digest (1975) 24 (12): Ni-222.
Published: 01 December 1975
... COLMONOY No. 4 is a nickel-base alloy containing chromium boride. It is recommended for hard surfacing parts to resist wear, heat, corrosion and galling. Deposits, which have only moderate hardness (Rockwell C 35-40), can be machined with carbide tooling. Also, deposits have fairly good...
Journal Articles
Alloy Digest (1993) 42 (6): Ni-433.
Published: 01 June 1993
... COLMONOY NO. 84 contains tungsten to harden the matrix and provide for good hard-facing. It is a nickel alternative to cobalt surfacing alloys, for service temperatures up to 1500 F. Boron and Silicon content provide better weldability at lower application temperatures. This datasheet provides...
Journal Articles
Alloy Digest (1995) 44 (11): Ni-489.
Published: 01 November 1995
... COLMONOY No. 69SC is a nickel-base hard surfacing alloy incorporating the qualities of Colmonoy No. 69 (Alloy Digest Ni-206, July 1974) with other enhancements. Its extended plastic range means that sagging and running of other-than-horizontal surfaces during finishing is virtually eliminated...
Journal Articles
Alloy Digest (1995) 44 (8): Co-98.
Published: 01 August 1995
... as well as powder metal forms. Filing Code: CO-98. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys hardness physical properties powder...