Skip Nav Destination
Close Modal
Search Results for
Colmonoy 805
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Colmonoy 805
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (12): Ni-233.
Published: 01 December 1998
... Colmonoy 805 is a nickel-chromium-boron alloy with coarse particles of chromium boride added to give it excellent sliding-type abrasion resistance. The alloy contains chromium boride in the matrix as large added particles. It is supplied only as a crushed powder for application with Colmonoy’s...
Abstract
View article
PDF
Colmonoy 805 is a nickel-chromium-boron alloy with coarse particles of chromium boride added to give it excellent sliding-type abrasion resistance. The alloy contains chromium boride in the matrix as large added particles. It is supplied only as a crushed powder for application with Colmonoy’s Fuseweld process. This datasheet provides information on composition, physical properties, microstructure, and elasticity. It also includes information on corrosion resistance as well as joining and powder metal forms.Filing Code: Ni-233. Producer or source: Wall Colmonoy Corporation. Originally published September 1976, revised December 1998.