Alloy Digest (2022) 71 (3): SS-1345.
Published: 01 March 2022
... Cleveland-Cliffs Thermak 17 is a ferritic stainless steel that is stabilized with both titanium and niobium. When given a high-temperature, final solution anneal, the alloy exhibits dramatic creep resistance. The dual stabilization prevents carbide sensitization exposure and makes the alloy...