Alloy Digest (2023) 72 (1): SS-1355.
Published: 01 January 2023
... Cleveland-Cliffs 444 is a low carbon, low nitrogen, dual stabilized ferritic stainless steel that provides pitting and crevice corrosion resistance superior to most ferritic stainless steels and some austenitic stainless steels. It is equivalent to Type 304 austenitic stainless steel in many...
Journal Articles
Alloy Digest (2022) 71 (3): SS-1345.
Published: 01 March 2022
... Thermak 17 was found to be superior to Cleveland-Cliffs 18 Cr-Cb and type 444 stainless steel in the temperature range 700 930 °C (1290 1705 °F). It was equivalent to Cleveland-Cliffs 15 Cr-Cb over the same temperature range. Thermal Fatigue Resistance. Cleveland-Cliffs Thermak 17 has shown, in limited...