Alloy Digest (1967) 16 (3): Cu-174.
Published: 01 March 1967
... Chromium Copper-182 is a copper-chromium corrosion resistant alloy which is softened by a high-temperature solution anneal and quench, and will improved acquire properties with a low temperature precipitation-hardening heat treatment. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1975) 24 (12): Cu-305.
Published: 01 December 1975
... Copper Alloy NO. 182 is an age-hardening type of alloy that combines relatively high electrical conductivity with good strength and hardness. It was formerly known as Chromium Copper and its applications include such uses as resistance-welding-machine electrodes, switch contacts and cable...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-589.
Published: 01 October 1993
... AMPCO-TRODE 182 is a chromium-copper alloy filler metal that has high conductivity with good strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-589. Producer or...
Journal Articles
Alloy Digest (1982) 31 (6): Cu-438.
Published: 01 June 1982
... ANACONDA Alloy 182 is a copper-base alloy containing nominally 0.85% chromium. It offers relatively high electrical conductivity, good strength and hardness and some resistance to softening at elevated temperatures. Among its uses are resistance welding electrodes, switchgear, and electrical and...
Journal Articles
Alloy Digest (1976) 25 (10): Cu-321.
Published: 01 October 1976
... avoided. Specification Equivalents: CDA Copper Alloy No. 182. ASTM F9, Chromium Copper. RWMA*, Group A, Class 2. *Resistance Welding Manufacturers Association. General Characteristics: Ampcoloy 97 is a heat-treatable (age-hardenable) cor- rosion-resistant ahoy combining high electrical con- ductivity and...
Journal Articles
Alloy Digest (1972) 21 (8): Cu-257.
Published: 01 August 1972
... MUELLER ALLOY 1820 (formerly MBCo 902) is a chromium-copper alloy with high electrical conductivity, high mechanical strength, and superior creep, fatigue and wear properties. It is used for resistance welding electrodes, switchgear, and electrical and electronic parts. This datasheet provides...
Journal Articles
Alloy Digest (1991) 40 (1): Ni-391.
Published: 01 January 1991
...-solution alloy that can be hardened only by cold working and it has excellent mechanical properties with good workability. Composition: Nickel Chromium Iron Carbon Manganese Sulfur Silicon Copper 72.0 min. 14.0-17.0 6.00- 10.0 0.15 max. 1.00 max. 0.015 max. 0.50 max. 0.50 max. Physical Constants: (Also see...
Journal Articles
Alloy Digest (1994) 43 (6): TS-527.
Published: 01 June 1994
..., x 1W Silicon 1.00 70-2OO F 6.10 70- 1000°F 7.38 SUlflU .003 max. 70-4OO F 6.66 70-1100°F 7.43 Chromium 5.3 70-6OO F 6.92 70- 1200°F 7.50 Molybdenum 1.4 70-8OO F 7.15 70-1300°F 7.56 VanadiUIll 1.0 70-9OO F 7.27 Thermal conductivity, Btu in/ft2+r*oF 70°F 180 1200°F 191 400°F 182 1300 F 192.5 800°F 184...
Journal Articles
Alloy Digest (1981) 30 (3): Ni-266.
Published: 01 March 1981
...!eBox8!z3 Upper Madair, New Jersq lNCONEL* Alloy 690 Korrosion-Resistant High-Chromium Nickel Alloy) INCONEL Alloy 690 is a wrought nickel-base alloy with excellent resistance to many au~osive. aqueous media and high-temperature atmos- pheres. It also has high strength, good metallurgical stability, and...
Journal Articles
Alloy Digest (1957) 6 (5): TS-58.
Published: 01 May 1957
... PRESSURDIE-2 is an intermediate chromium-tungsten-molybdenum hot die steel possessing excellent combination of properties particularly adapted for use in the aluminum extrusion industry. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It...
Journal Articles
Alloy Digest (1983) 32 (12): Ni-295.
Published: 01 December 1983
... HUNTINGTON alloy G is a nickel-chromium-iron alloy with additions of molybdenum, copper, copper and columbium. The alloy's composition provides an exceptionally useful combination of corrosion-resistance attributes. It is particularly suitable for handling reducing acids such as phosphoric and...
Journal Articles
Alloy Digest (1996) 45 (11): SS-660.
Published: 01 November 1996
... CLI-50A is a Korean 6 Mo superaustenitic stainless steel with improved corrosion resistance properties. The chromium additions have been increased up to 22% together with high nitrogen additions. The PREN value [%Cr] + 3.3 [%Mo] + 16[%N] is higher than 45. The alloy is copper free. This alloy is...
Journal Articles
Alloy Digest (2014) 63 (12): SS-1194.
Published: 01 December 2014
... chromium contents. URANUS® 926 (Super-Austenitic Stainless Steel) URANUS® 926 Chemical Composition, wt (Typical values) Carbon < 0.01 Chromium 20.5 Nickel 25.0 Molybdenum 6.3 Nitrogen 0.2 Copper 1.0 Sulfur 0.001 Iron bal PREN = [Cr%] + 3.3 [Mo %] + 16 [N%] 43 Physical Properties: Density, kg/m3 (lb/in.3...
Journal Articles
Alloy Digest (2004) 53 (5): SS-903.
Published: 01 May 2004
... Supermet 2205 is a manual metal arc (MMA) electrode with enhanced chromium, molybdenum, and nitrogen levels. It is used for welding standard 22% Cr duplex austenitic/ferritic stainless steels. This datasheet provides information on composition, microstructure, hardness, and tensile properties as...
Journal Articles
Alloy Digest (2014) 63 (10): SS-1187.
Published: 01 October 2014
... Chemical Composition, wt (Typical values) Carbon < 0.020 Chromium 27 Nickel 31 Molybdenum 3.5 Nitrogen 0.05 Copper 1.0 PREN = [Cr%] + 3.3 [Mo %] + 16 [N%] 39 Physical Properties: Density, kg/m3 (lb/in.3) 8000 (0.29) See Table 1. Mechanical Properties: Hardness, HV10 250 310 See Table 2. Impact Properties...
Journal Articles
Alloy Digest (1970) 19 (4): Ni-152.
Published: 01 April 1970
... solid-solution alloy with excellent high-temperature properties which make it attractive for many application in aerospace and process industries. *Registered Trademark of International Nickel. Composition: Nickel Chromium Iron Aluminum Carbon Manganese Sulfur Silicon Copper 60.5 23.0 14.1 1.35 0.05 0.5...
Journal Articles
Alloy Digest (1972) 21 (12): Ni-182.
Published: 01 December 1972
... ALTEMP 601 is a nickel-chromium solid-solution alloy with excellent high-temperature properties with good resistance to oxidizing, carburizing, and sulfur-containing environments. The properties make it attractive for applications in aerospace and process industries as well as automotive thermal...
Journal Articles
Alloy Digest (1967) 16 (10): SS-201.
Published: 01 October 1967
... readily formed and welded. Composition: Carbon Manganese Silicon Chromium Nickel t Co Titanium Copper Sulphur Iron 0.10 max. 1.5 max. 1.0 max. 19.0-22.0 30.0-34.0 0.75-1.50 0.50 max. 0.015 max. Remainder Physical Constants: Specific gravity Density, Ib/cu.in. Thermal coef. expansion, in/in/OF x 10-6 lOO...
Journal Articles
Alloy Digest (2003) 52 (11): Ni-617.
Published: 01 November 2003
... contents of chromium and aluminum, alloy 693 offers particularly good resistance to oxidation, carburization, sulfidation, and special resistance to metal dusting. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (2011) 60 (3): Ni-688.
Published: 01 March 2011
... NAS 600 is a nickel alloy with 14-17 chromium and has excellent oxidation resistance. The alloy is used extensively in heat treatment furnaces. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes...