Alloy Digest (1994) 43 (4): SA-473.
Published: 01 April 1994
... CHROME CORE 8 AND 8-FM alloys are controlled chemistry alloys for use in magnetic components where better corrosion resistance than iron and steel alloys is needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (5): SA-474.
Published: 01 May 1994
... CARPENTER CHROME CORE 12 AND 12-FM alloys are controlled alloys for use in magnetic components where better corrosion resistance than iron and steel alloys is needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...