Alloy Digest (2007) 56 (9): SS-996.
Published: 01 September 2007
... Chrome Core 13-XP alloy is a ferritic stainless steel with a controlled chemistry to improve corrosion resistance without significantly decreasing saturation induction in magnetic fields. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...