Alloy Digest (1954) 3 (2): Al-13.
Published: 01 February 1954
... CERALUMIN C is an age-hardenable aluminum alloy having good high temperature properties with exceptional fatigue strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on high...
Journal Articles
Alloy Digest (1958) 7 (2): Al-62.
Published: 01 February 1958
... CERALUMIN-D is an age-hardenable aluminum alloy having good high temperature properties with exceptional fatigue strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on heat...
Journal Articles
Alloy Digest (1960) 9 (8): Al-94.
Published: 01 August 1960
... CERALUMIN-B is an age-hardenable general purpose aluminum casting alloy having good high temperature properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on high...