Skip Nav Destination
Close Modal
Search Results for
Carpenter stainless no. 10
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 206 Search Results for
Carpenter stainless no. 10
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1954) 3 (4): SS-14.
Published: 01 April 1954
... CARPENTER STAINLESS NO. 10 is a stainless steel developed to overcome the manufacturing difficulties associated with the rapid work-hardening of conventional 18-8 stainless steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Abstract
View article
PDF
CARPENTER STAINLESS NO. 10 is a stainless steel developed to overcome the manufacturing difficulties associated with the rapid work-hardening of conventional 18-8 stainless steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-14. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1960) 9 (12): SS-111.
Published: 01 December 1960
... to that of Type 430, but it is not equal to that of Type 304, Type 305, or Carpenter No. 10. It is subject to intergranular corrosion and consequently should not be heated or cooled slowly in the range of 800-16500F. General Characteristics: Carpenter Stainless No. 12 is an austenitic chromium-nickel alloy steel...
Abstract
View article
PDF
Carpenter Stainless No. 12 is an austenitic chromium-nickel alloy designed for the manufacturer of cold-headed or cold forged parts. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-111. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1982) 31 (2): SS-401.
Published: 01 February 1982
... impact, ft-lb (J) 80000(552) 0 10 20 30 40 50 60 70 80 90 PERCENT COLD WORK Fig. 1 - Rate of work hardening of Carpenter Stainless Type 305 and two other popular austenitic cold-heading stainless steels (Carpenter Stainless No. 10 and Carpenter Stainless Custom Flo 302 HQL DOI: 10.31399/asm.ad.ss0401...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 305 has higher nickel content than the austenitic stainless steels considered to be in the 18% chromium-8% nickel category. Its high nickel content lowers the rate of strain hardening and, therefore, allows severe cold forming operations without the necessity of intermediate process anneals in comparison to the common 18-8 austenitic grades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-401. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1981) 30 (11): SS-395.
Published: 01 November 1981
... CARPENTER STAINLESS TYPE 405 is a 12% chromium stainless steel that does not harden appreciably. It was designed to allow its use in the as-welded condition. It is particularly desirable for welded applications which require finish machining. It has moderate tensile strength (70,000 psi...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 405 is a 12% chromium stainless steel that does not harden appreciably. It was designed to allow its use in the as-welded condition. It is particularly desirable for welded applications which require finish machining. It has moderate tensile strength (70,000 psi) in the fully annealed condition and resists corrosion in mild environments. It is used for parts and structures that cannot be annealed after welding. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-395. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1981) 30 (1): SS-379.
Published: 01 January 1981
... CARPENTER STAINLESS TYPE 303Se is a free-machining modification of the 18% chromium-8% nickel stainless steel. Type 303Se is used for all types of screw-machine products. This alloy is frequently used for machined parts which will be subjected to some cold forming in assembly operations...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 303Se is a free-machining modification of the 18% chromium-8% nickel stainless steel. Type 303Se is used for all types of screw-machine products. This alloy is frequently used for machined parts which will be subjected to some cold forming in assembly operations. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-379. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1978) 27 (7): SS-353.
Published: 01 July 1978
... CARPENTER STAINLESS 22Cr-13Ni-5Mn has very good corrosion resistance in combination with high strength. It has better corrosion resistance than AISI Type 316 stainless steel and approximately twice the yield strength. Carpenter 22Cr-13Ni-5Mn can be machined, cold worked and welded using the same...
Abstract
View article
PDF
CARPENTER STAINLESS 22Cr-13Ni-5Mn has very good corrosion resistance in combination with high strength. It has better corrosion resistance than AISI Type 316 stainless steel and approximately twice the yield strength. Carpenter 22Cr-13Ni-5Mn can be machined, cold worked and welded using the same equipment and methods used for the conventional AISI 300 series of stainless steels. It is nonmagnetic as annealed and after severe cold work. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-353. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1996) 45 (10): SS-658.
Published: 01 October 1996
... Carpenter Type 409Cb stainless steel is a 11% Cr steel stabilized with columbium (niobium). The alloy is used extensively in automobile exhast systems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Abstract
View article
PDF
Carpenter Type 409Cb stainless steel is a 11% Cr steel stabilized with columbium (niobium). The alloy is used extensively in automobile exhast systems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-658. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1977) 26 (10): SS-344.
Published: 01 October 1977
... CARPENTER STAINLESS 18-18 PLUS is an 18 chromium-18 manganese austenitic stainless steel which provides twice the yield strength of AISI Type 304 stainless steel and corrosion resistance similar to AISI Type 316 in some media. It has excellent ductility and toughness and good high-temperature...
Abstract
View article
PDF
CARPENTER STAINLESS 18-18 PLUS is an 18 chromium-18 manganese austenitic stainless steel which provides twice the yield strength of AISI Type 304 stainless steel and corrosion resistance similar to AISI Type 316 in some media. It has excellent ductility and toughness and good high-temperature strength. Although Carpenter 18-18 Plus contains no nickel, it is nonmagnetic both in the annealed condition and after severe cold forming. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-344. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1972) 21 (12): SS-284.
Published: 01 December 1972
... CARPENTER STAINLESS No. 404 is a hardenable, weldable, fully martensitic alloy for use in highly stressed parts at temperatures up to 1050 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also...
Abstract
View article
PDF
CARPENTER STAINLESS No. 404 is a hardenable, weldable, fully martensitic alloy for use in highly stressed parts at temperatures up to 1050 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-284. Producer or source: Carpenter. See also Alloy Digest SS-210, June 1968.
Journal Articles
Alloy Digest (1975) 24 (5): SS-310.
Published: 01 May 1975
... CARPENTER 21-12 is an austenitic chromium-nickel stainless steel which offers an excellent combination of high-temperature strength and corrosion resistance for exhaust valve applications. It is used widely as the head material in two-piece valves for both diesel and gasoline engines...
Abstract
View article
PDF
CARPENTER 21-12 is an austenitic chromium-nickel stainless steel which offers an excellent combination of high-temperature strength and corrosion resistance for exhaust valve applications. It is used widely as the head material in two-piece valves for both diesel and gasoline engines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-310. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1961) 10 (9): SS-121.
Published: 01 September 1961
... Carpenter Stainless 304+B is similar to conventional Type 304 with the addition of boron to give it a much higher thermal neutron absorption cross-section than other austenitic stainless steels. This datasheet provides information on composition, physical properties, hardness, elasticity...
Abstract
View article
PDF
Carpenter Stainless 304+B is similar to conventional Type 304 with the addition of boron to give it a much higher thermal neutron absorption cross-section than other austenitic stainless steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-121. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1994) 43 (2): SS-563.
Published: 01 February 1994
... Carpenter NeutroSorb and NeutroSorb PLUS are austenitic stainless steels modified with boron to increase the thermal neutron cross-section. These alloys are used for handling and storing radioactive material such as spent fuel. This datasheet provides information on composition, physical...
Abstract
View article
PDF
Carpenter NeutroSorb and NeutroSorb PLUS are austenitic stainless steels modified with boron to increase the thermal neutron cross-section. These alloys are used for handling and storing radioactive material such as spent fuel. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SS-563. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1982) 31 (1): SS-400.
Published: 01 January 1982
... CARPENTER STAINLESS TYPE 420F is a martensitic stainless that is easy to machine, grind and polish. In service it exhibits certain nongalling and nonseizing characteristics. It is used mainly for machined parts that require high hardness and good resistance to corrosion. Its applications include...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 420F is a martensitic stainless that is easy to machine, grind and polish. In service it exhibits certain nongalling and nonseizing characteristics. It is used mainly for machined parts that require high hardness and good resistance to corrosion. Its applications include pump shafts, gears, cams and pivots. This alloy is not usually recommended for vessels containing gases or liquid under high pressure. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-400. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1981) 30 (9): SS-391.
Published: 01 September 1981
... CARPENTER STAINLESS TYPE 443 is a heat-resisting chromium steel which stands up very well under destructive scaling conditions up to 1600 F (871 C). It is not subject to intergranular corrosion as a result of hot working, welding or continuous operation at elevated temperatures. Type 443...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 443 is a heat-resisting chromium steel which stands up very well under destructive scaling conditions up to 1600 F (871 C). It is not subject to intergranular corrosion as a result of hot working, welding or continuous operation at elevated temperatures. Type 443 is comparable to the 18-8 chromium-nickel stainless steels in resistance to both corrosion and scaling but is not as though as they are nor as hard at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-391. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1980) 29 (7): SS-275.
Published: 01 July 1980
... MPa psi MPa -- -- -- 60000 414 55000 379 52000 359 47000 324 40000 276 33000 228 32000 221 26000 179 20000 138 16500 114 11000 76 7000 48 8000 55 6000 41 - - 0.28 7750 7.75 0.11 0.46 6.5 x 10-6 11.7 x 10-6 343 570 Heat Treatment: Carpenter Stainless No. 5-F normally is furnished in the annealed...
Abstract
View article
PDF
CARPENTER STAINLESS No. 5-F is a modification of AISI Type 416 stainless steel and was designed for an optimum combination of machinability and corrosion resistance. It comprises a specially balanced analysis and is essentially non-hardenable. It is recommended for all screw-machine applications, particularly those involving intricate machining operations or where superior finishes are required as-machined. Its uses include valve trim, carburetor needles and many other screw-machine parts. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-275. Producer or source: Carpenter. Originally published July 1972, revised July 1980.
Journal Articles
Alloy Digest (1979) 28 (6): SS-366.
Published: 01 June 1979
... CARPENTER STAINLESS 18Cr-2Ni-12Mn is a high-manganese, nitrogen-strengthened austenitic stainless steel with an excellent combination of toughness, ductility, strength, fabricability and corrosion resistance. It provides substantially higher yield and tensile strengths than AISI Type 304...
Abstract
View article
PDF
CARPENTER STAINLESS 18Cr-2Ni-12Mn is a high-manganese, nitrogen-strengthened austenitic stainless steel with an excellent combination of toughness, ductility, strength, fabricability and corrosion resistance. It provides substantially higher yield and tensile strengths than AISI Type 304 and is comparable to Type 304 in corrosion resistance in many environments. It can be machined, cold worked, and welded using the same equipment and methods used for the conventional AISI 300 series austenitic stainless steels. It is nonmagnetic as annealed and after severe cold work. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-366. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1975) 24 (8): SS-316.
Published: 01 August 1975
... CARPENTER 21-12N is an austenitic chromium-nickel stainless steel for valves. It offers excellent high-temperature strength and hardness as well as corrosion resistance to combustion products. This alloy contains 0.15-0.25% nitrogen for increased high-temperature strength. It is widely used...
Abstract
View article
PDF
CARPENTER 21-12N is an austenitic chromium-nickel stainless steel for valves. It offers excellent high-temperature strength and hardness as well as corrosion resistance to combustion products. This alloy contains 0.15-0.25% nitrogen for increased high-temperature strength. It is widely used as the head material in two piece exhaust valves for both diesel and gasoline engines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-316. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1967) 16 (4): SS-193.
Published: 01 April 1967
... Carpenter Custom 455 is a low-carbon martensitic stainless steel that responds to precipitation-hardening. The single aging treatment produces exceptionally high yield strength with good ductility and toughness. It is suitable for applications requiring high strength and corrosion resistance...
Abstract
View article
PDF
Carpenter Custom 455 is a low-carbon martensitic stainless steel that responds to precipitation-hardening. The single aging treatment produces exceptionally high yield strength with good ductility and toughness. It is suitable for applications requiring high strength and corrosion resistance at temperatures up to 800 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-193. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1999) 48 (9): SS-763.
Published: 01 September 1999
... Carpenter Stainless Type 304HN is the high-nitrogen version of Type 304 and 304H stainless steels. Interstitial strengthening with both carbon and nitrogen provides this alloy with significantly higher yield and tensile strength as annealed. Typical applications include aerospace and power...
Abstract
View article
PDF
Carpenter Stainless Type 304HN is the high-nitrogen version of Type 304 and 304H stainless steels. Interstitial strengthening with both carbon and nitrogen provides this alloy with significantly higher yield and tensile strength as annealed. Typical applications include aerospace and power components, as well as marine shafting. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-763. Producer or source: Carpenter. See also Alloy Digest SS-368, October 1979.
Journal Articles
Alloy Digest (1979) 28 (10): SS-368.
Published: 01 October 1979
... CARPENTER STAINLESS TYPE 304HN is essentially a high-nitrogen version of AISI Type 304 stainless steel. By means of solid-solution strengthening, the nitrogen provides significantly higher yield strength and tensile strength as annealed than conventional Type 304, without adversely affecting...
Abstract
View article
PDF
CARPENTER STAINLESS TYPE 304HN is essentially a high-nitrogen version of AISI Type 304 stainless steel. By means of solid-solution strengthening, the nitrogen provides significantly higher yield strength and tensile strength as annealed than conventional Type 304, without adversely affecting ductility, corrosion resistance or nonmagnetic properties. Its applications include aircraft and aerospace components and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-368. Producer or source: Carpenter. See also Alloy Digest SS-763, September 1999.
1