... CARPENTER No. 883 is a 5% chromium hot work steel designed particularly for applications requiring extreme toughness combined with good red-hardness. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep. It also includes...
Journal Articles
Alloy Digest (1987) 36 (1): TS-469.
Published: 01 January 1987
... CARPENTER 883 PLUS is a premium quality die-casting die steel. It is electroslag remelted and this together with processing adaptations give it metallurgical consistency and improved isotropic properties. This datasheet provides information on composition, hardness, and tensile properties as well...
Journal Articles
Alloy Digest (1994) 43 (7): TS-529.
Published: 01 July 1994
... CARPENTER 883 PLUS is a 5% Chromium hot work die steel designed for applications requiring both toughness and good red-hardness. It achieves this with higher purity, homogeneity and greater structural integrity than standard AISI type H13. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1952) 1 (3): Al-3.
Published: 01 November 1952
... in/rev. yj$T&y a b 1/64-l/32 0.010 300-500 883 905 6 0.020 250-350 905 l/32 150-300 ii: 905 l/&l/4 l/32 SO-150 44A 883 (~otc: (a) is for average production and (b) is for cpnti~ production. Under propa conditions, the speeds shown may beimreaxd.Thcssdataap IyWhmtbetooIhasa front dcarancc angle of ll lo...
Journal Articles
Alloy Digest (1971) 20 (1): Ti-61.
Published: 01 January 1971
... the standpoint of optimum mechanical properties. Machinability: Rigid set-ups, good coolants and slow speeds are necessary for all machining operations on CARPENTER TITANIUM 66-2 Efficient and successful machining depends on tool life. Turning: Carbide tools such as K6, 883, and HA are recommended. High speed...
Journal Articles
Alloy Digest (1978) 27 (7): SS-353.
Published: 01 July 1978
... CARPENTER STAINLESS 22Cr-13Ni-5Mn has very good corrosion resistance in combination with high strength. It has better corrosion resistance than AISI Type 316 stainless steel and approximately twice the yield strength. Carpenter 22Cr-13Ni-5Mn can be machined, cold worked and welded using the same...
Journal Articles
Alloy Digest (1990) 39 (1): Fe-89.
Published: 01 January 1990
... as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-89. Producer or source: Carpenter. Producer or Source: Carpenter Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (1995) 44 (6): SS-596.
Published: 01 June 1995
... includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-596. Producer or source: Carpenter. Producer or Source: Carpenter Copyright © ASM International® 1996 1996 ASM International BioDur 316LS chemical composition corrosion...
Journal Articles
Alloy Digest (2005) 54 (1): SS-915.
Published: 01 January 2005
... Elongation, Reduction Condition work MPa ksi MPa ksi % of area, % Annealed n/a 448 65 841 122 39 58 Cold worked 5 586 85 855 124 32 66 35 883 128 1172 170 18 48 DOI: 10.31399/asm.ad.ss0915 eration by medical and surgical users in Europe. The premium electroslag remelted alloy is Carpenter s alternative...
Journal Articles
Alloy Digest (2000) 49 (12): SS-258.
Published: 01 December 2000
... Carpenter Custom 630 is a martensitic precipitation (age) hardening (PH) stainless steel offering high strength and hardness along with excellent corrosion resistance. It has good fabricating characteristics and can be age hardened by a single-step, low-temperature treatment. This datasheet...
Journal Articles
Alloy Digest (2000) 49 (5): SS-788.
Published: 01 May 2000
... Carpenter Project 7000 15Cr-5Ni offers strength and excellent corrosion resistance. Similar to Carpenter 15Cr-5Ni (Alloy Digest SS-346, January 1978) and Carpenter Custom 630 (Alloy Digest SS-258, revised December 2000), Project 7000 15Cr-5Ni stainless is intended for use when improved machining...
Journal Articles
Alloy Digest (1962) 11 (1): TS-113.
Published: 01 January 1962
... Cast Carpenter 883 Braebum Crucible Allegheny-Ludlum Latrobe Firth Sterling Bethlehem Jessop Uaivetsal Cyclops V&an-Kidd Columbia C8tpeIlte1 Forms Available: Billets, bars, forgings. Applications: Alumioum esmdimg dies, mandrel and d-y blocks; die casting dies for alnminutn; forged die inserts; brass...
Journal Articles
Alloy Digest (1961) 10 (11): TS-111.
Published: 01 November 1961
... Potomac M Pressurdie No 3 No. 883 Vanadium Firedie HWD No. 3 Dica B. Vanadium VDC Tbermold AV Vulcast Hotform 3 General Characteristics: Cutting Speeds, sfpm High Speed Cemented mSteA Carbide 58-66 240-280 48-54 200-230 40-46 180-195 34-38 150-170 Crucible Allegheny Ludlum Braebum Carpenter Columbia Fir...