1-8 of 8 Search Results for

Carpenter no. 5-317

Sort by
Journal Articles
Alloy Digest (1955) 4 (2): SA-27.
Published: 01 February 1955
... CARPENTER No. 5-317 is a nickel-chromium medium carbon steel for high combination of hardness and toughness in heat treated condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming...
Journal Articles
Alloy Digest (1992) 41 (2): SS-294.
Published: 01 February 1992
... CARPENTER 636 is a hardenable stainless steel designed for service up to 1200 F (649 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1992) 41 (2): SS-139.
Published: 01 February 1992
... CARPENTER 636 is a hardenable stainless steel designed for service up to 1200 F (649 C). It exhibits good resistance to scaling and oxidation in continuous service up to 1400 F (760 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1978) 27 (7): SS-353.
Published: 01 July 1978
... before cold drawing. DOI: 10.31399/asm.ad.ss0353 Copyright © ASM International® 1996 Table 5 - CORROSION DATA (Annealed condition) Average Corrosion Rate Environment Duration of Test Carpenter 22Cr-13Ni-5Mn AISI Type 3 16 10 w/o formic acid-boiling 3 periods - 48 hrs. ea. 50 w/o acetic acid-boiling 2.3...
Journal Articles
Alloy Digest (1974) 23 (7): SS-298.
Published: 01 July 1974
... in pickling tank. air-free. moderate aeitation at l20-14OoF for 43 hours) Material Corrosion Rate, Inches Per Year Carpenter Stainless No. ~-MC Nt, Cr. MO, Fe, Cb Alloy Carpenter Stainless 20 Stalniess Type 316 Stainless Type 317 Stainless Type 304L NI, Cr. MO. Fe Alloy NI. MO, Cr Alloy- *ASTM Designations...
Journal Articles
Alloy Digest (1987) 36 (1): SS-481.
Published: 01 January 1987
.... FERRALIUM alloy 255 1.6 < 0.08 AISI Type 316 28. 1.9 AISI Type 317 76. I.9 AISI Type 317 LM 97. I.1 ZOCb-3**Allov 41. 3.1 * I20 crevice; are possible. **Trademark of Carpenter Technologv Corp. Heat Treatment: ASTM .A 240. A 479. .A 789 and A 790. .ASME. S.4 2J0. S.4 479. S.4 89 and SA 790. .American Bureau...
Journal Articles
Alloy Digest (2012) 61 (3): Ni-695.
Published: 01 March 2012
... temperature, °C (°F) Average stress for rupture life, MPa (ksi) 100 h 1000 h 10,000 h 593 (1100) 537 (78) 427 (62) 345 (50) 649 (1200) 393 (57) 317 (46) 255 (37) 760 (1400) 207 (30) 152 (22) 110 (16) 816 (1500) 145 (21) 96 (14) 69 (10) 871 (1600) 90 (13) 55 (8) 34 (5) 927 (1700) 62 (9) 41 (6) 982 (1800) 41...
Journal Articles
Alloy Digest (1977) 26 (6): SS-340.
Published: 01 June 1977
... at 1325oF - 7190C - and air cooled) Test Rupture in 100 Hours Rupture in 1000 Hours Temperature Stress Elongation Stress Elongation oF oc psi (MPa) (4D), ? o psi (MPa) (4D), % -- 1000 538 99000 (683) 3 88000 (607) 3 1100 593 81500 (562) 3 71500 (493) 1200 649 61000 (421) 5 46000 (317) i 1300 704 44500 (307...