Alloy Digest (1967) 16 (4): SS-193.
Published: 01 April 1967
... Carpenter Custom 455 is a low-carbon martensitic stainless steel that responds to precipitation-hardening. The single aging treatment produces exceptionally high yield strength with good ductility and toughness. It is suitable for applications requiring high strength and corrosion resistance...
Journal Articles
Alloy Digest (2012) 61 (3): SS-1117.
Published: 01 March 2012
... 455® stainless steel. Products Available: Forms manufactured: wire Applications: Its initial use in medical and surgical applications is in the manufacture of surgical needle wire as a replacement for Custom 455 stainless. Producer: Carpenter Specialty Alloys Reading, PA 19612 USA Tel: (610) 208-2000...
Journal Articles
Alloy Digest (1998) 47 (5): SS-716.
Published: 01 May 1998
.... It develops high strength along with fracture toughness and resistance to stress-corrosion cracking. Custom 465 is a trademark, while Custom 455 is a registered trademark of Carpenter Technology Corporation. PH 13-8Mo is a registered trademark of Armco. Inc. Chemical Composition, wt (Type Analysis) carbon h&t...
Journal Articles
Alloy Digest (2006) 55 (9): SS-974.
Published: 01 September 2006
... CARPENTER CUSTOM 475 chemical composition corrosion-resistant alloys ductility hardness heat treatability machinability physical properties tensile strength workability wrought stainless steel UNS S24000 Chemical Composition, wt (Type Analysis) Carbon 0.01 max Manganese 0.50 max. Phosphorus...
Journal Articles
Alloy Digest (1982) 31 (2): SS-401.
Published: 01 February 1982
... impact, ft-lb (J) 80000(552) 0 10 20 30 40 50 60 70 80 90 PERCENT COLD WORK Fig. 1 - Rate of work hardening of Carpenter Stainless Type 305 and two other popular austenitic cold-heading stainless steels (Carpenter Stainless No. 10 and Carpenter Stainless Custom Flo 302 HQL DOI: 10.31399/asm.ad.ss0401...