Alloy Digest (1994) 43 (1): SS-561.
Published: 01 January 1994
... CARPENTER STAINLESS TYPE 430F SOLENOID QUALITY offers much of the properties of 430 stainless steel, but through composition and processing maintains consistently high magnetic permeability and low residual induction. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1977) 26 (3): SS-337.
Published: 01 March 1977
... ferritic alloy specifically developed for solenoid valve magnetic core components and relay parts which must operate in corrosive environments. Car- penter 430FR exhibits the following three advantages over 430F Solenoid Quality (Rockwell B 75/82 or 82/91) stainless and other commercially available 430F...