Alloy Digest (1966) 15 (6): SS-182.
Published: 01 June 1966
... Carpenter Stainless 20Cb-3 is an austenitic stainless steel designed for improved resistance to sulfuric acid. It finds wide use in all phases of the chemical industry. It has good mechanical properties and comparative ease of fabrication. Columbium stabilizes the alloy to minimize carbide...
Journal Articles
Alloy Digest (2010) 59 (3): SS-1059.
Published: 01 March 2010
... resistance of this product is slightly higher when working at room temperature. Weldability: The weldability is similar to any ordinary austenitic stainless steel. Preheating and postheating are not necessary. The producer recommends using higher-alloyed material such as Carpenter 20Cb-3 or Hastelloy C-type...
Journal Articles
Alloy Digest (1987) 36 (1): SS-481.
Published: 01 January 1987
... of Attacked Crevices* FERRALIUM alloy 255 0 AlSl Type 317 LM 20 Alloy No. 904L 23 AlSl Type 317L I6 20Cb-3** alloy 24 AISI Type 316 24 *Maximum possible number of crevice **Trademark of Carpenter Technolog) t Perforated. Maximum Depth of Penetration mils mm 0 I2 I9 77 76 76 was 24. orp. 0 0.30 0.48 2.0 1.9...