1-20 of 222 Search Results for

Carpenter STAINLESS no. 2

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1956) 5 (9): SS-47.
Published: 01 September 1956
... CARPENTER STAINLESS No. 2 is a high carbon heat-treatable chromium stainless steel equivalent to AISI Type 420; while No. 2-FM is the free-machining modification equivalent to AISI Type 420-F. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1979) 28 (8): SS-367.
Published: 01 August 1979
... Carpenter Stainless No. 2 Mold Steel is a 13% chromium steel ideally suited for long-run molding jobs. It is specifically used for protection against the following corrosive conditions: (1) Rusting of cavities when machines are shut down or molds are stored, (2) Rusting of mold cavities when using...
Journal Articles
Alloy Digest (1982) 31 (2): SS-401.
Published: 01 February 1982
... bars, wire and wire rods, strip and tubular products. Applications: Carpenter Stainless Type 305 is used: (1) In severe cold-working operations, (2) Where the finished part must remain virtually nonmagnetic after severe cold working, (3) For deep-drawn parts such as eyelets, (4) For cold-headed bolts...
Journal Articles
Alloy Digest (1985) 34 (3): SS-459.
Published: 01 March 1985
... laboratory experimental work and improved manufac- turing techniques. It has significantly; better machinability than the conventional AISI Type 416 in three respects: (I) 100 to 2009c longer tool life. (2) 15% faster machtmng speeds and (3) Improved finishes. Carpenter Project 70 Stainless Type 416...
Journal Articles
Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... CARPENTER 20Mo-6 is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting and stress-corrosion cracking in chloride environments and is also resistant to oxidizing media. Its good resistance to corrosion has been...
Journal Articles
Alloy Digest (1983) 32 (9): SS-432.
Published: 01 September 1983
... CARPENTER STAINLESS 302HQ-FM, a modification of Carpenter Stainless Custom Flo 302HQ, has excellent cold headability plus machinability approaching that of AISI Type 303 stainless steel. It is designed primarily for cold-headed parts that are to be drilled, slotted, broached, etc; in addition...
Journal Articles
Alloy Digest (1984) 33 (12): SS-455.
Published: 01 December 1984
... be machined at speeds of 120! 150 surface feet per minute (37146 meters per minute). Hot Working: Carpenter Stainless Type 430F should be heated uniformly to 150011600°F (816!871 C) and then taken to the forging temperature of 1950 2 100 F ( 1066 I 1 149 C) as rapidly as possible. Do not soak at the forging...
Journal Articles
Alloy Digest (1981) 30 (1): SS-379.
Published: 01 January 1981
... CARPENTER STAINLESS TYPE 303Se is a free-machining modification of the 18% chromium-8% nickel stainless steel. Type 303Se is used for all types of screw-machine products. This alloy is frequently used for machined parts which will be subjected to some cold forming in assembly operations...
Journal Articles
Alloy Digest (1974) 23 (7): SS-298.
Published: 01 July 1974
... CARPENTER STAINLESS No. 7-Mo is a two-phase alloy consisting of a ferritic matrix with pools of austenite. It has high resistance to stress-corrosion cracking and pitting, and good general corrosion resistance in many environments. Its principal use is for tubing and pipe in heat exchangers...
Journal Articles
Alloy Digest (1981) 30 (9): SS-391.
Published: 01 September 1981
... CARPENTER STAINLESS TYPE 443 is a heat-resisting chromium steel which stands up very well under destructive scaling conditions up to 1600 F (871 C). It is not subject to intergranular corrosion as a result of hot working, welding or continuous operation at elevated temperatures. Type 443...
Journal Articles
Alloy Digest (1984) 33 (10): SS-452.
Published: 01 October 1984
... CARPENTER STAINLESS TYPE 440A is a high-carbon chromium steel designed to provide stainless properties at high hardness. It has sufficient corrosion resistance in the annealed condition to permit its use in mild environments. In some respects it behaves similarly to tool steels. It can...
Journal Articles
Alloy Digest (1980) 29 (7): SS-275.
Published: 01 July 1980
... CARPENTER STAINLESS No. 5-F is a modification of AISI Type 416 stainless steel and was designed for an optimum combination of machinability and corrosion resistance. It comprises a specially balanced analysis and is essentially non-hardenable. It is recommended for all screw-machine applications...
Journal Articles
Alloy Digest (1977) 26 (10): SS-344.
Published: 01 October 1977
... CARPENTER STAINLESS 18-18 PLUS is an 18 chromium-18 manganese austenitic stainless steel which provides twice the yield strength of AISI Type 304 stainless steel and corrosion resistance similar to AISI Type 316 in some media. It has excellent ductility and toughness and good high-temperature...
Journal Articles
Alloy Digest (1978) 27 (7): SS-353.
Published: 01 July 1978
... CARPENTER STAINLESS 22Cr-13Ni-5Mn has very good corrosion resistance in combination with high strength. It has better corrosion resistance than AISI Type 316 stainless steel and approximately twice the yield strength. Carpenter 22Cr-13Ni-5Mn can be machined, cold worked and welded using the same...
Journal Articles
Alloy Digest (2005) 54 (2): SS-916.
Published: 01 February 2005
... Carpenter Stainless Type 304LN is a common, often used austenitic stainless steel. This data sheet emphasizes its use as rebar. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1984) 33 (4): SS-443.
Published: 01 April 1984
...-mm) rounds. Steel annealed at 19OO F ( 1038 C)] Tensile strength. psi (MPal 85000 (586) Yield strength (0.2% offset). psi (MPa) 35000 (241) Elongation (2 in.: 50.8 mm). 9 60 Reduction of area. 9 70 Brine11 hardness 150 lzod impact. ft-lb (J) 110 (149) *Carpenter Stainless Type 302 is an excellent...
Journal Articles
Alloy Digest (1979) 28 (6): SS-366.
Published: 01 June 1979
.... Hydrochloric acid at 1400F (6000 max. - 2 minutes - water rinse. Machinability: Carpenter 18Cr-2Ni-12Mn has a machinability rating about 35% of AISI B1112, or about 70% of AISI Type 316 stainless steel. Slow to moderate speeds, moderate feeds and rigid tools are recommended. Chips tend to be tough and stringy...
Journal Articles
Alloy Digest (2005) 54 (4): SS-924.
Published: 01 April 2005
.../Ferritic Duplex Stainless Steel) Carpenter 2205 Stainless is a common, often used austenitic/ferritic duplex stainless steel. This data sheet emphasizes its use as rebar. Table 2 Charpy V-notch (CVN) Impact Data for Rebar at Various Test Temperatures Impact strength, Test temperature Charpy V-notch °C °F J...
Journal Articles
Alloy Digest (1979) 28 (10): SS-368.
Published: 01 October 1979
... CARPENTER STAINLESS TYPE 304HN is essentially a high-nitrogen version of AISI Type 304 stainless steel. By means of solid-solution strengthening, the nitrogen provides significantly higher yield strength and tensile strength as annealed than conventional Type 304, without adversely affecting...
Journal Articles
Alloy Digest (1995) 44 (9): SS-608.
Published: 01 September 1995
... CARPENTER 7-Mo PLUS is a duplex stainless steel of austenite in a ferrite matrix. It is superior to 300 series stainless steels like types 304 and 316 in strength, corrosion, pitting and stress-corrosion cracking resistance (to chlorides). Typical applications are heat exchangers in the chemical...