Alloy Digest (1990) 39 (5): Ni-383.
Published: 01 May 1990
... Carpenter Nickel 205 alloy exhibits an excellent combination of mechanical, electrical and corrosion resistant properties. It is resistant to oxidation. It is ferromagnetic below 680 F (360 C). The alloy is produced to closely controlled composition including small additions of magnesium...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (4): Ni-550.
Published: 01 April 1999
... joinability machinability physical properties tensile properties workability thermal properties UNS N10276 CARPENTER ALLOY C-276 (Nickel Alloy) Carpenter alloy C-276 is a Ni-Mo-Cr-W alloy with good fabricability. The alloy is balanced to provide excellent corrosion resistance to a vari- ety...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (4): SS-711.
Published: 01 April 1998
... thermal properties UNS - - DIGEST - QCopynght 1998, Ask4 htematkmat Au rigm reservedDatashownam~,nottobe uaedbrrspedficeiionortinat&aign. CARPENTER TYPE 204=CU DATA ON WORLD WlDE METALS AND ALLOYS CARPENTER TYPE 2044U (Low-Nickel Austenitic Stainless Steel) Carpenter type 204-Cu is a low-nickel...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (1): Ni-400.
Published: 01 January 1992
... by: Alloy Digest. Ix I201 -677.9161 27 CanibId SIreel. Orange. N.J. 07050 I U.S.A. TOPHEL@ ALLOY, NIAL ALLOY, NICROSIL/NISIL ALLOYS, 20 & 19 ALLOYS (Nickel-Base Thermocouple Alloys) TOPHEL@ Alloy and NIAL Alloy are respectively the positive and negative thermoelements for ISA* Type K thermocouples. NICROSIL...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (10): Ni-5.
Published: 01 October 1971
... Carpenter HYMU 80 is an unoriented 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability and maximum permeability with minimum hysteresis loss at low magnetic field strengths. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (2): SS-1084.
Published: 01 February 2011
... PLUS (Martensitic Age-Hardening Stainless Steel) CARPENTER TOURALLOY 230 PLUS Chemical Composition, wt (Typical analysis) Carbon 0.05 Manganese 0.1 Phosporus 0.010 max Sulfur 0.008 max Silicon 0.1 Chromium 12.25 13.25 Nickel 7.50 8.50 Molybdenum 2.00 2.50 Aluminum 0.90 1.35 Nitrogen 0.01 Iron bal...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (6): Ti-128.
Published: 01 June 2002
... Carpenter CP Titanium Grade 4 is the highest-strength grade of the unalloyed grades 1-4. It competes with steels and nickel alloys with its combination of corrosion resistance, fatigue properties, and high strength. This datasheet provides information on composition, physical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (9): SS-974.
Published: 01 September 2006
... 0.015 max Sulfur 0.010 max Silicon 0.50 max Chromium 10.50 11.50 Nickel 0`7.5 8.50 Molybdenum `4.50 5.50 Cobalt `8.00 9.00 Aluminum `1.00 1.50 Iron bal Physical Properties: Density, kg/m3 (lb/in.3) Annealed 7972 (0.288) Conditions H950, H975, H1000, 7999 (0.289) H1025, H1050 Condition H1100 8055 (0.291...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (2): Cu-803.
Published: 01 February 2012
... Manganese 0.30 Nickel 1.00 Copper bal Physical Properties: Density, kg/m3 (lb/in.3) 8940 (0.3230) Mean specific heat, 20 ºC (68 ºF), J/kg·K (Btu/lb·ºF) 377 (0.090) Thermal conductivity, W/m·K (Btu/(hr·ft·ºF)) 21 (12) Electrical resistivity, 25 ºC (77 ºF), m ( circular-mil/ft) 0.04 (27.00) Temperature...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (9): SS-432.
Published: 01 September 1983
... is a registered trademark of Carpenter Technology Corporation. Composition: Carbon 0.06 max. Manganese 2.00 max. Phosphorus 0.040 max. Sulfur 0.20 max. Silicon 1.00 max. Chromium 16.00-19.00 Nickel 9.00-l 1.00 Copper 1.20-2.40 Iron Remainder Type Analysis Physical Constants: Density. Ib/cu/in. kglculm Specific...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (8): SS-757.
Published: 01 August 1999
... BioDur 108 alloy is an austenitic alloy but is essentially nickel-free. It contains a very high content of nitrogen to maintain the austenitic structure. The major uses for this alloy are in the biochemical industry for products such as implantable orthopedic components. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (5): TS-813.
Published: 01 May 2021
... CarTech AerMet-for-Tooling is a low-carbon, cobalt-nickel-chromium-molybdenum, alloy tool steel that exhibits high strength and high hardness together with exceptional ductility and toughness. This alloy is designed for components that require a hardness of about 53–55 HRC along with very high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (12): Ni-397.
Published: 01 December 1991
... ~h119#.ALby~.kAU~hk1-. Pt&wmdby: AloyD@6!, InI% 1201-677-6161 ~&y#$g&gm-- PYROMET ALLOY M-252 27 Canlield Slrwl. Chqe, NJ. 07050 I USA (Precipitation Hardening Nickel-Base High-Temperature Alloy) PYROMET alloyM-252 was designed for use in highly stressed parts operating at temperatures up to 16OO F (871...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1952) 1 (4): SA-4.
Published: 01 December 1952
... CARPENTER No. 5-876 is a nickel-chromium-molybdenum triple alloy steel for hard-tempered and for tough-tempered applications. It is a cold melt, grain controlled, electric furnace steel. This datasheet provides information on composition, hardness, and tensile properties. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (2): Ni-536.
Published: 01 February 1998
... physical properties PYROMET 31V tensile properties workability thermal properties UNS N07031 ecopvriohr 1998, ASM Intemarional. All nghk tmemDetasllcwnem~,nottobs usdlbrs~t orfinsl&?sign. PYROMET@31V DATA ON WORLD WIDE METALS AND ALLOYS PYROMET@31V (Valve Steel) Filing Code: Ni-636 m Nickel Alloy u...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (3): Co-134.
Published: 01 March 2021
... Carbon (UNS R30035)(b) Manganese Silicon 0.02 0.025 Table 2 Thermal and electrical properties Phosphorus Sulfur 0.15 0.15 Coefficient of Chromium linear thermal Nickel 0.15 0.15 expansion(a) Thermal Molybdenum conductivity Iron 0.015 0.015 Temperature Electrical resistivity Titanium Btu/ Boron 0.010...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (7): SA-21.
Published: 01 July 1954
... AISI 8740 is a medium-carbon, nickel, chromium, molybdenum alloy steel of the oil hardening type. It has good hardenability and desirable toughness. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also...