Alloy Digest (2005) 54 (6): Fe-137.
Published: 01 June 2005
... Carpenter Glass Sealing 42-6 alloy has been used for sealing to Corning 0120 glass. A special thermal treatment develops a tightly adherent oxide beneficial to obtaining hermetic seals. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...