Alloy Digest (2013) 62 (11): SS-1160.
Published: 01 November 2013
... Carpenter CTS BD1 alloy is a high-carbon chromium steel that provides stainless properties with high hardness and excellent wear resistance. In terms of hardness and wear resistance, this alloy behaves very similarly to tool steels. This alloy attains a hardness of 58–60 HRC when heat treated...