Alloy Digest (2009) 58 (6): Fe-148.
Published: 01 June 2009
... Carpenter AerMet 340 Alloy possesses high hardness and strength while exhibiting exceptional toughness and ductility, and can be considered for a variety of automotive, racing, aerospace, and defense applications. This datasheet provides information on composition, physical properties, hardness...