Alloy Digest (1992) 41 (2): SS-294.
Published: 01 February 1992
... CARPENTER 636 is a hardenable stainless steel designed for service up to 1200 F (649 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1992) 41 (2): SS-139.
Published: 01 February 1992
... CARPENTER 636 is a hardenable stainless steel designed for service up to 1200 F (649 C). It exhibits good resistance to scaling and oxidation in continuous service up to 1400 F (760 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1998) 47 (2): Ni-536.
Published: 01 February 1998
... information on composition, physical properties, elasticity, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and machining. Filing Code: Ni-536. Producer or source: Carpenter...