Alloy Digest (1995) 44 (8): Ni-484.
Published: 01 August 1995
... on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-484. Producer or source: Carpenter. Producer or Source: Carpenter Copyright Ā© ASM InternationalĀ® 1996 1996 ASM International Carpenter 20Mo-4 chemical composition corrosion-resistant...
Journal Articles
Alloy Digest (1984) 33 (5): SS-444.
Published: 01 May 1984
... and reagent grade concentrated phosphoric acid. Field samples were exposed to wet process superphosphoric acid in a two stage evaporator. see Table 4 for details. Intergranular Corrosion Resistance: Carpenter 20Mo-6 stainless is melted with low carbon to provide a high level of resistance to...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-556.
Published: 01 July 1999
.... Examples of laboratory and simulated field environments in which U-bend type test specimens of 20Mo-6 HS have been evaluated include the data shown in Tables 4 and 5. Pitting and Crevice Corrosion Resistance. Cold-drawn wire products representing several heats of 20Mo-6 HS stainless have been evaluated for...