1-1 of 1

Search Results for Carpenter 15-15HS MAX stainless

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2007) 56 (3): SS-988.
Published: 01 March 2007
.... CARPENTER 15-15HS® MAX STAINLESS Filing Code: SS-988 Stainless Steel March 2007 CARPENTER 15-15HS® MAX STAINLESS (Austenitic Stainless Steel) 15-15HS MAX stainless is an austenitic alloy strengthened by both nitrogen and high manganese. It has a low permeability and can be considered for nonmagnetic drill...