1-10 of 10 Search Results for

Carlson Alloy Nitronic 50

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2008) 57 (12): SS-1025.
Published: 01 December 2008
... Carlson Alloy Nitronic 50 has corrosion resistance superior to 316L and 317L with twice the yield strength at ambient temperatures. It possesses good mechanical properties at both elevated and subzero temperatures, and retains low magnetic permeability even after severe cold working or at subzero...
Journal Articles
Alloy Digest (2005) 54 (6): SS-931.
Published: 01 June 2005
... Carlson alloy Nitronic 33 has twice the yield strength of 304 stainless with comparable corrosion resistance. The low magnetic permeability of the alloy is retained after severe cold working. The resistance to chloride stress-corrosion cracking is superior to Type 304. Nitronic 33 has excellent...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1029.
Published: 01 February 2009
... CARLSON ALLOY NITRONIC 60 is a galling- and wear-resistant austenitic stainless steel that provides a significantly lower-cost alternative to cobalt-bearing and high-nickel alloys. Corrosion resistance is superior to 304 in most media. Approximately twice the yield strength of 340 and 316...
Journal Articles
Alloy Digest (2015) 64 (10): SS-1228.
Published: 01 October 2015
... Carlson Alloy Nitronic 40 has corrosion resistance superior to 316L and 317L with twice the yield strength at ambient temperatures. Possesses good mechanical properties at both elevated and sub-zero temperatures. Retains low magnetic permeability even after severe cold working or at sub-zero...
Journal Articles
Alloy Digest (2013) 62 (4): SS-1142.
Published: 01 April 2013
.... Filing Code: SS-1142. Producer or source: Electralloy, a Division of G.O. Carlson Inc.. See also Alloy Digest SS-324, January 1976. Producer or Source: Electralloy, a Division of G.O. Carlson Inc. Copyright © ASM International® 2013 2013 ASM International chemical composition corrosion...
Journal Articles
Alloy Digest (2018) 67 (9): SS-1294.
Published: 01 September 2018
... Code: SS-1294. Producer or source: Electralloy, a Division of G.O. Carlson Inc.. Producer or Source: Electralloy, a Division of G.O. Carlson Inc. Copyright © ASM International® 2018 2018 ASM International chemical composition corrosion-resistant alloys Electralloy Nitronic 32...
Journal Articles
Alloy Digest (1998) 47 (5): SS-715.
Published: 01 May 1998
... 1998 ASM International chemical composition corrosion-resistant alloys ELECTRALLOY NITRONIC 50 ELECTRALLOY NITRONIC 50 HS heat treatability joinability machinability physical properties workability thermal properties UNS S20910 - DIGEST - DATA ON WORLD WlDE METALS AND ALLOYS Filina...
Journal Articles
Alloy Digest (1998) 47 (6): SS-721.
Published: 01 June 1998
..., such as wear rings and lobes. Ekcualloy Nitronic 60 is one of the most effective wear and galling resistant alloys for bridge pins and other critical construction applications. Producer: Ele.ctralloy A G.O. Carlson, Inc. Company Oil City, PA 16301 (814) 6784100 (800) 458-7273 (814) 678-4172 (fax) ISSN: 002...
Journal Articles
Alloy Digest (2018) 67 (11): SS-1297.
Published: 01 November 2018
... and high temperature performance, and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-1297. Producer or source: Electralloy, a Division of G.O. Carlson Inc.. Producer or Source: Electralloy, a Division of G.O. Carlson Inc. Copyright © ASM International® 2018...
Journal Articles
Alloy Digest (2018) 67 (10): SS-1295.
Published: 01 October 2018
... as joining. Filing Code: SS-1295. Producer or source: Electralloy, a Division of G.O. Carlson Inc.. Producer or Source: Electralloy, a Division of G.O. Carlson Inc. Copyright © ASM International® 2018 2018 ASM International chemical composition corrosion-resistant alloys ductility Electralloy...