Skip Nav Destination
Close Modal
Search Results for
Carilloy T-1
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-3 of 3 Search Results for
Carilloy T-1
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1955) 4 (1): SA-25.
Published: 01 January 1955
... CARILLOY T-1 is a low-carbon complex alloy steel used where high levels of yield strength and toughness are required. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance...
Abstract
View article
PDF
CARILLOY T-1 is a low-carbon complex alloy steel used where high levels of yield strength and toughness are required. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SA-25. Producer or source: United States Steel Corporation.
Journal Articles
Alloy Digest (1961) 10 (1): SA-108.
Published: 01 January 1961
... & Forgings hfIL-T-18165 (3) Ships, Class 2, Tube & Pipe MIL-I-16286B (-2) Ships, Class C, Tubes, Seamless ASTM A387, Grade D. Plates ASTM A155, Grade 2 1, 4Cr, Pipe ASTM A335, Grade P22, Pipe ASTM A369, Grade FP22, Pipe ASTM A199, Grade T22, Tubes ASTM AZOO, Grade 122, Tubes ASTM A213, Grade T22. Tubes ASTM...
Abstract
View article
PDF
U.S.S. CARILLOY 21/4 Cr-1Mo is a low alloy oxidation and corrosion resistant steel suitable for moderately high (900-1100 F) temperature use. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-108. Producer or source: United States Steel Corporation.
Journal Articles
Alloy Digest (1959) 8 (9): SA-89.
Published: 01 September 1959
... CARILLOY 1% Cr-1/2% Mo is a low alloy oxidation, corrosion and graphitization resistant steel suitable for moderately high (900-1100 deg. F.) temperature use. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Abstract
View article
PDF
CARILLOY 1% Cr-1/2% Mo is a low alloy oxidation, corrosion and graphitization resistant steel suitable for moderately high (900-1100 deg. F.) temperature use. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-89. Producer or source: United States Steel Corporation.