... CarTech Micro-Melt 440-XH is an air-hardening, high-carbon, high chromium, corrosion resistant alloy tool steel that is produced by the powder metallurgy process. It can be considered as either a high hardness Type 440C martensitic stainless steel or a corrosion- resistant Type D2 alloy tool steel...