Alloy Digest (2011) 60 (9): SA-632.
Published: 01 September 2011
... CarElso 70 (355) is clean steel for pressure equipment in mild sour service. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-632. Producer or source...
Journal Articles
Alloy Digest (2009) 58 (1): SA-588.
Published: 01 January 2009
... CarElso 70 HIC is a steel alloy with special melt practice producing a clean, normalized pressure vessel material with excellent resistance to hydrogen-induced cracking (HIC). This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2009) 58 (1): SA-590.
Published: 01 January 2009
... CarElso 70 SOHIC is a steel alloy with special melt practice producing a pressure vessel material with excellent resistance to stress-oriented hydrogen-induced cracking (SOHIC). This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (2011) 60 (10): SA-635.
Published: 01 October 2011
... of heat treatment after forming. Weldability: Consumables used for the welding of CarElso 60/65 must correspond to the following standards: SMAW GMAW FCAW SAW wire flux EN EN499 EN440 EN 758 EN756/EN 760 E42 XXXH5 G 42 XX T 42 XX H5 S 42 XX AWS A5-5 A5-18 A5-20 A5-17 E 70xx ER 70 S-x E 7xT5-x F7P4-Exxx...
Journal Articles
Alloy Digest (2008) 57 (9): SA-584.
Published: 01 September 2008
... CarElso 60/65 HIC is a steel alloy with special melt practice producing a pressure vessel material with excellent resistance to hydrogen-induced cracking (HIC). This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information...