Alloy Digest (1979) 28 (3): TS-346.
Published: 01 March 1979
... CYCLOPS SCK is a cold-work tool steel with a balanced composition to provide air hardening and an optimum combination of toughness, wear resistance and minimum distortion during heat treatment. Typical applications are shear blades, trimming dies and forming rolls, including grade rolls...