Alloy Digest (1966) 15 (6): Cu-164.
Published: 01 June 1966
... CUNISIL-647 is a copper-nickel-silicon precipitation-hardening alloy having high strength, hardness, wear and corrosion resistance. Typical applications include electrical hardware and fasteners. This datasheet provides information on composition, physical properties, hardness, elasticity...