Alloy Digest (1980) 29 (4): SS-372.
Published: 01 April 1980
... CRYOTECH 302 is a new, cryogenically processed stainless steel wire with the same composition as AISI Type 302. The cryogenic processing gives tensile and torsional properties that are independent of wire diameter (thus simplifying spring design calculations) and markedly greater than those of...