... CRUCIBLE XM 19 Stainless is a nitrogen-strengthened, low-carbon austenitic stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosion resistance than AISI Type 316 with approximately twice the yield strength. It can be welded, machined...