Alloy Digest (1980) 29 (6): Ti-77.
Published: 01 June 1980
... CRUCIBLE C-120AV is an alpha-beta type titanium-base alloy with 120,000 psi minimum yield strength in the annealed condition. It has good forming characteristics, is weldable with proper shielding and can be heat treated to high strength levels by solution treating and aging. Its many applications...