Alloy Digest (1980) 29 (12): SS-378.
Published: 01 December 1980
... CRUCIBLE 316 PLUS is a non-hardenable austenitic chromium-nickel steel with superior corrosion and heat resisting qualities. Better machinability than that of standard AISI Type 316 stainless is obtained by the use of balanced chemistry and special manufacturing techniques. This grade is non...
Journal Articles
Alloy Digest (1982) 31 (9): SS-414.
Published: 01 September 1982
... CRUCIBLE XM 19 Stainless is a nitrogen-strengthened, low-carbon austenitic stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosion resistance than AISI Type 316 with approximately twice the yield strength. It can be welded, machined...