Alloy Digest (1991) 40 (6): SS-521.
Published: 01 June 1991
... CRUCIBLE 17Cr-4Ni SUPER-X is a precipitation-hardening martensitic stainless steel which develops high strength and hardness after relatively simple heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as...