1-6 of 6 Search Results for

CRU-WEAR

Sort by
Journal Articles
Alloy Digest (2001) 50 (11): TS-592.
Published: 01 November 2001
... CRU-WEAR is an air hardening tool steel with wear resistance greater than D2 and toughness approaching A2. Applications include blades, punches and dies. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating...
Journal Articles
Alloy Digest (2005) 54 (3): TS-615.
Published: 01 March 2005
... in full-size laboratory bearing component tests. CPM VIM CRU 20 has high attainable hardness, excellent hot hardness, fine carbide size, uniform carbide distribution, and excellent wear resistance. Producer: Crucible Service Centers Divisional Headquarters Camillus, NY (315) 487-0800 (800) 365-1185 (315...
Journal Articles
Alloy Digest (1958) 7 (1): Ti-14.
Published: 01 January 1958
... REM-CRU C-135AMo is a titanium-base alloy having good time-temperature-stress stability and deep hardenability. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness, creep, and fatigue. It also...
Journal Articles
Alloy Digest (1958) 7 (5): Ti-16.
Published: 01 May 1958
... REM-CRU A-70 is the grade of unalloyed titanium used where higher strength is required. It is specified for many moderately stressed aircraft parts. (Formerly known as RC-70.) This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (1959) 8 (7): Ti-20.
Published: 01 July 1959
... atmosphere should be oxidixing to minimize hydrogen comamination.) SURFACE HARDENING: Nitriding in Pure nitrogen is ektive for case depths of 0.0035 after 16 hours at 16OOOF. Carburizing in a mixture of W% pro. pane in argon at 1750.18OOOF. for 6.8 hours pro duces a very wear resistant case of 0.0001...
Journal Articles
Alloy Digest (1973) 22 (7): Pb-10.
Published: 01 July 1973
... 0.20 totaL The ahoy grades and compositions are from ASTM B 23. Physical Constants: Alloy7 Alloy8 Density, Ib/cu in. Specific gravity Melting point, oF Solidus Specific heat caIrl OOOC) ThermaI coei. expansion/oC (20-10~ Thermal conductivity, ~al/cru~/a/cm/~ (At 20┬░C) Electrical resistivity, microhm-cm...