Alloy Digest (1982) 31 (7): SS-411.
Published: 01 July 1982
... CRONIFER 2328 is a titanium-stabilized, high-chromium and high-nickel austenitic stainless steel with additions of molybdenum and copper. It exhibits good corrosion resistance against sulfuric and phosphoric acids. Also, it has good resistance against pitting and stress-corrosion cracking...