Alloy Digest (1973) 22 (5): TS-254.
Published: 01 May 1973
... Cromo-High V is a 5% chromium-molydbenum-vanadium tool steel that is used widely in the die-casting industry. It has high red-hardness with good resistance to abrasion and heat checking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1977) 26 (2): TS-313.
Published: 01 February 1977
...) High resistance to shock, (3) Easy to machine and (4) Good resistance to heat-checking. It will withstand drastic cooling from maximum operating temperatures. The hot-working and heat-treating characteristics of Cromo-V can be summerized as follows: Forging: Annealing: Preheating: Hardening: Tempering...
Journal Articles
Alloy Digest (1962) 11 (1): TS-113.
Published: 01 January 1962
... 240-280 l/l6 l/32 48-54 200.230 l/8 l/32 40-46 MO-195 l/4 l/32 34-38 120-170 l Woldman 81 Gibbons: Machinability & Machiaiog of Metals. Specification Equivalent: AISI Type HI3 SAE Type H13 Pressuredie 3 Nu-Die V Potomac M V.D.C. HWD No. 3 Cromo-High V Dica B. Vaaadium Thermold AV Vulcast Vanadium Die...
Journal Articles
Alloy Digest (1964) 13 (1): TS-142.
Published: 01 January 1964
... by . . ErqpemgAllqrDidat.Inc. Upper Montdair, New Ja=v CROMO-N tool steel is a low-carbon, high-chromium grade, specially developed to provide optimum re- sistance to heat-checking during service at elevated temperatures. It is recommended for aluminum die casting dies, extrusion press tooling, aluminum and copper forging...