Alloy Digest (1970) 19 (12): Mo-11.
Published: 01 December 1970
... CRM MOLYBDENUM-50 RHENIUM is a high-melting-point alloy for applications such as electronics tube components, electrical contacts, thermionic converters, thermocouples, heating elements and rocket thrusters. All products are produced by powder metallurgy. This datasheet provides information on...
Journal Articles
Alloy Digest (1970) 19 (8): Re-1.
Published: 01 August 1970
... CRM RHENIUM is a commercially pure, high-melting-point metal for applications such as electronics tube components, electrical contacts, thermionic converters, thermocouples, heating elements and rocket thrusters. All products are produced by powder metallurgy. This datasheet provides information...
Journal Articles
Alloy Digest (1971) 20 (11): W-17.
Published: 01 November 1971
... sintered billets are warm rolled to intermediate gages and then either cold or warm rolled to finished sizes. This alloy is easier to work than pure tungsten or tungsten-25 rhenium, but not as easy to work as molybdenum-50 rhenium. It is normally supplied in the fully recrystallized form; this is its most...