Skip Nav Destination
Close Modal
Search Results for
CP-W 800
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 30 Search Results for
CP-W 800
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (6): SA-816.
Published: 01 June 2018
... CP-W 800, 900, 1000 are part of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar...
Abstract
View article
PDF
CP-W 800, 900, 1000 are part of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles, cross members, body reinforcements, bumper bars, and chassis parts. This datasheet provides information on composition and tensile properties. It also includes information on heat treating. Filing Code: SA-816. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (4): SA-843.
Published: 01 April 2019
... CP-W 800 is one of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...
Abstract
View article
PDF
CP-W 800 is one of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles, cross members, body reinforcements, bumper bars, and chassis parts. This datasheet provides information on composition and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: SA-843. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (3): SA-841.
Published: 01 March 2019
... CP-W 660 is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles...
Abstract
View article
PDF
CP-W 660 is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles, cross members, body reinforcements, bumper bars, and chassis parts. This datasheet provides information on composition and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: SA-841. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (7): SA-849.
Published: 01 July 2019
... CP-K 900Y 1180T is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...
Abstract
View article
PDF
CP-K 900Y 1180T is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles, cross members, body reinforcements, bumper bars, and chassis parts. This datasheet provides information on composition and tensile properties. It also includes information on forming and heat treating. Filing Code: SA-849. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (8): Ti-181.
Published: 01 August 2021
... to 425 °C (800 °F), and in intermittent service at 540 °C (1000 °F). Chemical Composition Mechanical Properties Element Composition, wt%(a) See Tables 1 and 2. Carbon UPM CP Titanium Grade 4 Corrosion Resistance Oxygen Grade 4 (UNS R50700) Nitrogen UPM CP Titanium Grade 4 is highly resistant to many...
Abstract
View article
PDF
UPM CP Titanium Grade 4 (UNS R50700) is an unalloyed commercially pure titanium. It is the strongest of the four unalloyed commercially pure (CP) titanium grades, with a minimum yield strength of 480 MPa (70 ksi). This material exhibits good ductility, moderate formability, and excellent resistance to corrosion and corrosion fatigue. It can be used in continuous service at temperatures up to 425 °C (800 °F), and in intermittent service at 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-181. Producer or source: United Performance Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (6): SA-848.
Published: 01 June 2019
... CP-K 570Y780T is one of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...
Abstract
View article
PDF
CP-K 570Y780T is one of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles, cross members, body reinforcements, bumper bars, and chassis parts. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating. Filing Code: SA-848. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (9): Ti-182.
Published: 01 September 2021
... ATI CP Grade 16 Titanium is an unalloyed titanium grade that contains 0.04–0.08% Pd. This Pd-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 16 Titanium is used in applications requiring excellent corrosion...
Abstract
View article
PDF
ATI CP Grade 16 Titanium is an unalloyed titanium grade that contains 0.04–0.08% Pd. This Pd-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 16 Titanium is used in applications requiring excellent corrosion resistance in chemical processing or in storage applications where the media is mildly reducing or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-182. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (2): Ti-175.
Published: 01 February 2021
... correct parameters have been established, ATI tolerances similar to those attainable with stainless steel are 1000 Six PPG Place possible. The cold formability of ATI CP Grade 7 Titanium is Pittsburgh, Pennsylvania 15222, USA less than that of CP Grade 1 and Grade 11 titanium. Tel: +1 800 289 7454 Web...
Abstract
View article
PDF
ATI CP Grade 7 Titanium is an unalloyed titanium grade that contains 0.12–0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 7 Titanium is used in applications requiring excellent corrosion resistance in chemical processing or storage applications where the media is mildly reducing or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, tensile properties and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-175. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (6): Ti-179.
Published: 01 June 2021
... ATI CP Grade 11 Titanium is an unalloyed titanium grade that contains 0.12-0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 11 Titanium is used in applications requiring excellent...
Abstract
View article
PDF
ATI CP Grade 11 Titanium is an unalloyed titanium grade that contains 0.12-0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 11 Titanium is used in applications requiring excellent corrosion resistance in chemical processing or storage applications where the media is mildly reducing or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-179. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (6): Ti-167.
Published: 01 June 2020
... UPM CP Titanium Grade 3 (UNS R50550) is an unalloyed commercially pure titanium that exhibits moderate strength (higher strength than that of Titanium Grade 2), along with excellent formability and corrosion resistance. It offers the highest ASME allowable design stress of any commercially pure...
Abstract
View article
PDF
UPM CP Titanium Grade 3 (UNS R50550) is an unalloyed commercially pure titanium that exhibits moderate strength (higher strength than that of Titanium Grade 2), along with excellent formability and corrosion resistance. It offers the highest ASME allowable design stress of any commercially pure grade of titanium, and can be used in continuous service up to 425 °C (800 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-167. Producer or source: United Performance Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (1): Ti-162.
Published: 01 January 2020
... ATI corrosion-resistant commercially pure (CP) titanium represents a family of unalloyed (Grades 1, 2, 3 and 4) and palladium alloyed (Grades 7, 11, 16 and 17) CP titanium that is produced as plate, sheet and strip. It is the material of choice for many corrosive chemical environments, including...
Abstract
View article
PDF
ATI corrosion-resistant commercially pure (CP) titanium represents a family of unalloyed (Grades 1, 2, 3 and 4) and palladium alloyed (Grades 7, 11, 16 and 17) CP titanium that is produced as plate, sheet and strip. It is the material of choice for many corrosive chemical environments, including oxidizing chloride solutions (such as seawater) and chlorine-based bleaches. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Ti-162. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (10): Ti-131.
Published: 01 October 2003
... Titanium bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 3760 (0.136) Melting point, °C (°F) 1668 (3035) Coefficient of linear thermal expansion, 9.9 (5.5) 20 427 °C (68 800 °F), 10 6/K (10 6/°F) Thermal conductivity, 204 °C (400 °F), 17 (9.8) W/m K (Btu/(ft h °F)) Mechanical...
Abstract
View article
PDF
ASTM B 367 GRADE C-3 is a commercially pure titanium casting alloy. For the most part, titanium casting alloys are based on traditional wrought product compositions. Several data sheets for commercially pure (CP) grades of wrought titanium alloys have been published in Alloy Digest. This data sheet covers one of the most popular grades in cast form. The cast version is used because it is cost effective and as corrosion resistant as the wrought form. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: TI-131. Producer or source: The International Titanium Association.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (11): Ti-132.
Published: 01 November 2003
...: (Approximate) Density, kg/m3 (lb/in.3 ) 3760 (0.136) Melting point, °C (°F) 1668 (3035) Coefficient of linear thermal 9.9 (5.5) expansion, 20 427 °C (68 800 °F), 10 6/K (10 6/°F) Thermal conductivity, 204 °C (400 °F), 17 (9.8) W/m K (Btu/(ft h °F)) Mechanical Properties: Tensile strength, min, MPa (ksi...
Abstract
View article
PDF
ASTM B 367 GRADE Ti-Pd8A is commercially pure titanium casting alloy with a small palladium addition. For the most part, titanium casting alloys are based on traditional wrought product compositions. The small palladium addition to this grade improves corrosion resistance while not changing any of the physical or mechanical properties over the similarly composed commercially pure (CP) grade. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: TI-132. Producer or source: International Titanium Association.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (4): Ti-177.
Published: 01 April 2021
... °F) 9.6 20 100 °C (5.3) (a) Maximum values unless indicated otherwise. (b) Source: ASTM B348/B348M:2019 (68 212 °F) and ASTM B863:2019. (c) Source: ASTM F67:2013(2017). (d) Maximum hydrogen 9.7 content for billet is 0.0100% (5.4) Mechanical Properties Thermal W/(m K) 17 Tensile properties at room...
Abstract
View article
PDF
L. Klein Titan Grade 2 is an unalloyed, commercially pure titanium grade. It is the most widely used commercially pure titanium grade. It offers a combination of moderate strength and good ductility, with outstanding corrosion resistance in many challenging service environments. L. Klein Titan Grade 2 can operate in continuous service up to 425 °C (800 °F) and in intermittent service up to 540 °C (1005 °F). This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance and wear resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-177. Producer or source: L. Klein SA.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (11): Ti-115.
Published: 01 November 2000
... Allegheny Ludlum CP chemically pure titanium alloys feature low density and high strength-to-weight ratio. They are suitable for many corrosive chemical environments, including oxidizing chloride solutions, seawater, and chlorine-based bleaches. This datasheet provides information on composition...
Abstract
View article
PDF
Allegheny Ludlum CP chemically pure titanium alloys feature low density and high strength-to-weight ratio. They are suitable for many corrosive chemical environments, including oxidizing chloride solutions, seawater, and chlorine-based bleaches. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming and joining. Filing Code: TI-115. Producer or source: Allegheny Ludlum Corporation. Originally published September 2000, corrected November 2000.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (6): Ti-156.
Published: 01 June 2014
..., RT, W/m·K (Btu/(h·ft·°F)) 15.9 (9.2) Specific heat, RT, J/kg·K (Btu/lb·°F) 534 (0.128) Diffusivity, RT, m2/s (ft2/s) 6.61 × 10 4 (7.1 × 10 6) Mean coefficient of thermal expansion, 10 6/K (10 6/°F) 25 100 °C (77 212 °F) 9.6 (5.3) 25 500 °C (77 932 °F) 10.4 (5.8) 25 800 °C (77 1472 °F) 10.0 (5.5...
Abstract
View article
PDF
Timetal Exhaust XT is a lean alloy, but exhibits good corrosion resistance and higher strength than needed for automotive exhaust. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming. Filing Code: Ti-156. Producer or source: Timet.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (3): TS-19.
Published: 01 March 1954
..., wear re&anm, and armion rrsisrpncc It is P ASM QSVJS IV-B CYFC JOY- Composition: Nominal Range EEt Y-z: cp:-y.g chromium X& 5:00%0 vanadium Molyh&rmm 1:10 0.75-1.00 Iron +zzi%i5 PROPERTlES HARDNESS DATA Tempering T-y- 1000 1025 1050 1100 1150 1200 Heat Treutmenk ANNEAL: Hear co 1650 deg. F. fucnace...
Abstract
View article
PDF
PRESSURDIE-3, developed particularly for injection and compression molding, has high compression strength, wear resistance, and corrosion resistance. It is a ASM Class IV-B type alloy. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-19. Producer or source: Continental Copper & Steel Industries Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (5): Ni-708.
Published: 01 May 2013
...) , 10 6/K (10 6/°F) , W/m·K (Btu/(h·ft·°F)) cp, J/kg·K (Btu/lb·°F) a, m2/s (ft2/s) 20 (68) 13.8 (8.0) 445.9 (0.107) 2.8 × 10 6 (3.0 × 10 5) 100 (212) 14.0 (7.8) 15.1 (8.7) 464.1 (0.111) 3.1× 10 6 (3.3 × 10 5) 200 (392) 14.5 (8.1) 16.8 (9.7) 483.9 (0.116) 3.4 × 10 6 (3.7 × 10 5) 300 (572) 15.0 (8.3...
Abstract
View article
PDF
Centralloy G4879 Micro is a cast nickel alloy with very good high-temperature properties. The alloy has carbides in a uniform dispersion that impede dislocation movement. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on casting, machining, and joining. Filing Code: Ni-708. Producer or source: Schmidt & Clemens Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (11): Ni-683.
Published: 01 November 2010
...) Method Bulk density, , kg/m3 (lb/in.3) Specific heat, cp, J/kg · K (Btu/lb · ºF) Thermal diffusivity, , mm2/s (10 5 · ft2/s) Thermal conductivity, , W/m · K (Btu/h · ft · ºF) 25 (77) ASTM E1461 7880 (0.28) 4750 (1.1) 2.81 (3.02) 10.5 (6.1) 200 (392) ASTM E1461 7830 (0.28) 5250 (1.2) 3.28 (3.05) 13.5...
Abstract
View article
PDF
Deloro 50 EXV is also called Deloro 53. It is a self-fluxing alloy for abrasion and corrosion resistance. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties as well as fracture toughness. It also includes information on wear resistance as well as powder metal forms. Filing Code: Ni-683. Producer or source: Deloro Stellite Company Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1952) 1 (4): CI-1.
Published: 01 December 1952
... for 5 hours, &a & h4mlakd sationThi&lcrs,in. sationThi~in. 1 3 6 1 3 6 E 83ooo 76ooo 75ooo ZG 7O0O0 zz zio 45 2:o 180 16 180 12 5 180 1 Or DIGEST CARPENTER No. 5-876 RltgcokfA-8 -w DECRMEER 19E2 DATA ON WORLD WIDE METALS AND ALLOYS Publisbcd by Eogineaing Alloys Digesf Inc upper W New J-w CARPENTER...
Abstract
View article
PDF
NODULOY is a magnesium inoculated ductile cast iron in which the graphite is in the nodular form. It offers excellent castability, high mechanical properties, good machinability, pressure tightness, high modulus, and excellent shock resistance. It has extraordinary high ductility in the annealed state. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: CI-1. Producer or source: Dominion Wheel & Foundries Ltd.