Skip Nav Destination
Close Modal
Search Results for
CP-W 1000
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 24 Search Results for
CP-W 1000
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (5): SA-845.
Published: 01 May 2019
... CP-W 1000 is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...
Abstract
View article
PDF
CP-W 1000 is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles, cross members, body reinforcements, bumper bars, and chassis parts. This datasheet provides information on composition and tensile properties. It also includes information on heat treating and joining. Filing Code: SA-845. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (6): SA-816.
Published: 01 June 2018
... CP-W 800, 900, 1000 are part of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar...
Abstract
View article
PDF
CP-W 800, 900, 1000 are part of a family of complex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements,profiles, cross members, body reinforcements, bumper bars, and chassis parts. This datasheet provides information on composition and tensile properties. It also includes information on heat treating. Filing Code: SA-816. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (9): Ti-182.
Published: 01 September 2021
... or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermit- tent service up to 540 °C (1000 °F). Chemical Composition Mechanical Properties Composition, wt%(a) See Tables 1 and 2. The mechanical properties of ATI CP Grade 16 Titanium are comparable...
Abstract
View article
PDF
ATI CP Grade 16 Titanium is an unalloyed titanium grade that contains 0.04–0.08% Pd. This Pd-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 16 Titanium is used in applications requiring excellent corrosion resistance in chemical processing or in storage applications where the media is mildly reducing or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-182. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (2): Ti-175.
Published: 01 February 2021
... or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermit- tent service up to 540 °C (1000 °F). Chemical Composition Property Unit At Value RT Composition, wt%(a) Thermal W/(m K) 16 conductivity (Btu/(h·ft·°F)) RT (9.25)(c) Element ATI Grade 7...
Abstract
View article
PDF
ATI CP Grade 7 Titanium is an unalloyed titanium grade that contains 0.12–0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 7 Titanium is used in applications requiring excellent corrosion resistance in chemical processing or storage applications where the media is mildly reducing or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, tensile properties and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-175. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (6): Ti-179.
Published: 01 June 2021
... between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermit- tent service up to 540 °C (1000 °F). Chemical Composition Mechanical Properties Composition, wt%(a) See Tables 1 and 2. The mechanical properties of ATI CP Grade 11 Titanium are comparable to those...
Abstract
View article
PDF
ATI CP Grade 11 Titanium is an unalloyed titanium grade that contains 0.12-0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 11 Titanium is used in applications requiring excellent corrosion resistance in chemical processing or storage applications where the media is mildly reducing or fluctuates between oxidizing and reducing. It can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-179. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (8): Ti-100.
Published: 01 August 1992
... © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys CP TITANIUM TIMET GRADES Ti-100A CP TITANIUM TIMET GRADES Ti-35A CP TITANIUM TIMET GRADES Ti-50A CP TITANIUM TIMET GRADES Ti-65A CP TITANIUM TIMET GRADES Ti-75A ductility elasticity heat...
Abstract
View article
PDF
TIMET GRADES Ti-35A, Ti-50A, Ti-65A, Ti-75A, Ti-100A unalloyed titanium offer good ductility and cold formability, good to excellent weldability, and good to excellent corrosion resistance in neutral to oxidizing environments, including chlorides. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-100. Producer or source: Titanium Metals Corporation (Timet).
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (8): Ti-181.
Published: 01 August 2021
... to 425 °C (800 °F), and in intermittent service at 540 °C (1000 °F). Chemical Composition Mechanical Properties Element Composition, wt%(a) See Tables 1 and 2. Carbon UPM CP Titanium Grade 4 Corrosion Resistance Oxygen Grade 4 (UNS R50700) Nitrogen UPM CP Titanium Grade 4 is highly resistant to many...
Abstract
View article
PDF
UPM CP Titanium Grade 4 (UNS R50700) is an unalloyed commercially pure titanium. It is the strongest of the four unalloyed commercially pure (CP) titanium grades, with a minimum yield strength of 480 MPa (70 ksi). This material exhibits good ductility, moderate formability, and excellent resistance to corrosion and corrosion fatigue. It can be used in continuous service at temperatures up to 425 °C (800 °F), and in intermittent service at 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-181. Producer or source: United Performance Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (6): Ti-167.
Published: 01 June 2020
... UPM CP Titanium Grade 3 (UNS R50550) is an unalloyed commercially pure titanium that exhibits moderate strength (higher strength than that of Titanium Grade 2), along with excellent formability and corrosion resistance. It offers the highest ASME allowable design stress of any commercially pure...
Abstract
View article
PDF
UPM CP Titanium Grade 3 (UNS R50550) is an unalloyed commercially pure titanium that exhibits moderate strength (higher strength than that of Titanium Grade 2), along with excellent formability and corrosion resistance. It offers the highest ASME allowable design stress of any commercially pure grade of titanium, and can be used in continuous service up to 425 °C (800 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-167. Producer or source: United Performance Metals.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (1): Ti-162.
Published: 01 January 2020
... ATI corrosion-resistant commercially pure (CP) titanium represents a family of unalloyed (Grades 1, 2, 3 and 4) and palladium alloyed (Grades 7, 11, 16 and 17) CP titanium that is produced as plate, sheet and strip. It is the material of choice for many corrosive chemical environments, including...
Abstract
View article
PDF
ATI corrosion-resistant commercially pure (CP) titanium represents a family of unalloyed (Grades 1, 2, 3 and 4) and palladium alloyed (Grades 7, 11, 16 and 17) CP titanium that is produced as plate, sheet and strip. It is the material of choice for many corrosive chemical environments, including oxidizing chloride solutions (such as seawater) and chlorine-based bleaches. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Ti-162. Producer or source: ATI.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (5): Fe-25.
Published: 01 May 1964
... forces. Con LOIS, WC/W.. Yillllatls par Pound Carpenter i4iph Permcabiliry 4 7-Transiormer Grade- Normal Core Loss Curves 2t D. C.. M cps. and :00 cps jlne ilux excitation. rmg lam- Inations 0006 and U.OIY thick Hydrogen annealed IIJO F. 4 hours. furnace cooled After this material is given a low...
Abstract
View article
PDF
CARPENTER HIGH PERMEABILITY 49 is an iron-nickel alloy of high magnetic permeability recommended for magnetic and electrical equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating. Filing Code: Fe-25. Producer or source: Carpenter.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (3): TS-19.
Published: 01 March 1954
..., wear re&anm, and armion rrsisrpncc It is P ASM QSVJS IV-B CYFC JOY- Composition: Nominal Range EEt Y-z: cp:-y.g chromium X& 5:00%0 vanadium Molyh&rmm 1:10 0.75-1.00 Iron +zzi%i5 PROPERTlES HARDNESS DATA Tempering T-y- 1000 1025 1050 1100 1150 1200 Heat Treutmenk ANNEAL: Hear co 1650 deg. F. fucnace...
Abstract
View article
PDF
PRESSURDIE-3, developed particularly for injection and compression molding, has high compression strength, wear resistance, and corrosion resistance. It is a ASM Class IV-B type alloy. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-19. Producer or source: Continental Copper & Steel Industries Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (5): Ni-708.
Published: 01 May 2013
...) , 10 6/K (10 6/°F) , W/m·K (Btu/(h·ft·°F)) cp, J/kg·K (Btu/lb·°F) a, m2/s (ft2/s) 20 (68) 13.8 (8.0) 445.9 (0.107) 2.8 × 10 6 (3.0 × 10 5) 100 (212) 14.0 (7.8) 15.1 (8.7) 464.1 (0.111) 3.1× 10 6 (3.3 × 10 5) 200 (392) 14.5 (8.1) 16.8 (9.7) 483.9 (0.116) 3.4 × 10 6 (3.7 × 10 5) 300 (572) 15.0 (8.3...
Abstract
View article
PDF
Centralloy G4879 Micro is a cast nickel alloy with very good high-temperature properties. The alloy has carbides in a uniform dispersion that impede dislocation movement. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on casting, machining, and joining. Filing Code: Ni-708. Producer or source: Schmidt & Clemens Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1952) 1 (4): CI-1.
Published: 01 December 1952
... for 5 hours, &a & h4mlakd sationThi&lcrs,in. sationThi~in. 1 3 6 1 3 6 E 83ooo 76ooo 75ooo ZG 7O0O0 zz zio 45 2:o 180 16 180 12 5 180 1 Or DIGEST CARPENTER No. 5-876 RltgcokfA-8 -w DECRMEER 19E2 DATA ON WORLD WIDE METALS AND ALLOYS Publisbcd by Eogineaing Alloys Digesf Inc upper W New J-w CARPENTER...
Abstract
View article
PDF
NODULOY is a magnesium inoculated ductile cast iron in which the graphite is in the nodular form. It offers excellent castability, high mechanical properties, good machinability, pressure tightness, high modulus, and excellent shock resistance. It has extraordinary high ductility in the annealed state. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: CI-1. Producer or source: Dominion Wheel & Foundries Ltd.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (11): Ti-184.
Published: 01 November 2021
... any toxic ions into aqueous solutions, thus helping to prevent pollution. 0.1 Crevice Corrosion. Bibus Metals Titan Grade 1 has excellent 0.4 resistance to crevice corrosion in salt solutions and generally outperforms stainless steels. Unalloyed CP titanium typically bal bal do not suffer crevice...
Abstract
View article
PDF
Bibus Metals Titan Grade 1 is an unalloyed commercially pure titanium. It has the highest purity, lowest strength, and best ductility and formability of the four ASTM unalloyed titanium grades. This grade has excellent resistance to corrosion in highly oxidizing to mildly reducing environments, including chlorides. Bibus Metals Titan Grade 1 can be used in continuous service up to 425 °C (795 °F) and in intermittent service up to 540 °C (1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ti-184. Producer or source: Bibus Metals AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (12): TS-144.
Published: 01 December 1991
.../200 w 93) 70/400 wm4) 70/800 (211427.1 70/1200 (21/648) Coefficient x 1W per OF (per C) 6.0 (10.8) 6.4 (11.5) 7.0 (12.6) 7.3 (13.1) Test Temperature OF ( Cl 70 ( 21) 200 ( 93) 400 wJ4) 600 (316) 800 (427) 1000 (538) Modulus psix 106 (MPax Iv) 30.0 (20.7) 29.0 (20.0) 27.0 (18.6) 28.5 (19.7) 27.5 (19.0...
Abstract
View article
PDF
DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade. It is produced by consumable electrode vacuum melting which provides superior cleanliness, elimination of dissolved gases and preferred ingot structure. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as heat treating. Filing Code: TS-144. Producer or source: Latrobe Steel Company. Originally published as Dynaflex, February 1964, revised December 1991.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (3): P-33.
Published: 01 March 1992
... ULTEM 4001 is an unreinforced polyetherimide resin with an internal lubricant. It is wear resistant and it has a reduced coefficient of friction. See also ULTEM 4000 (Alloy Digest CP-21, March 1992) for reinforced resin properties. ULTEM 4001 is available in opaque colors only. This datasheet...
Abstract
View article
PDF
ULTEM 4001 is an unreinforced polyetherimide resin with an internal lubricant. It is wear resistant and it has a reduced coefficient of friction. See also ULTEM 4000 (Alloy Digest CP-21, March 1992) for reinforced resin properties. ULTEM 4001 is available in opaque colors only. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness. It also includes information on wear resistance as well as casting and powder metal forms. Filing Code: P-33. Producer or source: G. E. Plastics.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (7): Cp-16.
Published: 01 July 1990
... (23°C) fi-WYJ/W 1 .o (50) 1.6 (80) Unnotched, l/8 , 73OF (23OC) ft-lbs/m (J/m) 8.0 (400) 8.0 (400) Shear strength, ultimate D732 ~0 14.0 (97) 14.0 (97) Rockwell hardness D785 Ml 14 Ml14 Taber abrasion, CS 17, lkg D1044 Mg wt 104 1000 cycles 17 20 ULTEM 6202 14.0 (97) 5.0 (35) NA 6 21.0 (145) 9.0 (60...
Abstract
View article
PDF
ULTEM 6100 and 6200 are glass reinforced and ULTEM 6202 is a mineral filled copolymer resin. For properties of the unreinforced resin, ULTEM 6000, see Alloy Digest P-27, June 1991. These are high temperature materials that are particularly suitable for military electrical components which must survive 200 C testing. This datasheet provides information on physical properties, hardness, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance. Filing Code: Cp-16. Producer or source: G. E. Plastics.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (11): Ni-683.
Published: 01 November 2010
...) Method Bulk density, , kg/m3 (lb/in.3) Specific heat, cp, J/kg · K (Btu/lb · ºF) Thermal diffusivity, , mm2/s (10 5 · ft2/s) Thermal conductivity, , W/m · K (Btu/h · ft · ºF) 25 (77) ASTM E1461 7880 (0.28) 4750 (1.1) 2.81 (3.02) 10.5 (6.1) 200 (392) ASTM E1461 7830 (0.28) 5250 (1.2) 3.28 (3.05) 13.5...
Abstract
View article
PDF
Deloro 50 EXV is also called Deloro 53. It is a self-fluxing alloy for abrasion and corrosion resistance. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties as well as fracture toughness. It also includes information on wear resistance as well as powder metal forms. Filing Code: Ni-683. Producer or source: Deloro Stellite Company Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (5): Ti-147.
Published: 01 May 2010
... ºF), W/m · K (Btu/h · ft ºF) 21.8 (12.6) Coefficient of thermal expansion, 10-6 /K (10-6/ºF) 20 100 ºC (68 212 ºF) 8.6 (4.8) 20 300 ºC (68 572 ºF) 9.5 (5.3) 20 500 ºC (68 932 ºF) 9.7 (5.4) Magnetic permeability Nonmagnetic Mechanical Properties: Elastic modulus(a), GPa (psi) 105 120 (15.2 17.4...
Abstract
View article
PDF
TIMETAL 65A is a general purpose grade of commercially pure titanium that has excellent corrosion resistance to highly oxidating to mildly reducing environments, including chlorides, and an excellent strength-to-weight ratio. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: TI-147. Producer or source: Timet.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (8): Ni-709.
Published: 01 August 2013
.... Centralloy is a registered trademark of Schmidt + Clemens GmbH. Table 1 Physical properties , °C (°F) , 10 6/K (10 6/°F) E, GPa (106 psi) c p , J/kg·K (Btu/lb·°F) , W/m·K (Btu/(h·ft·°F)) 20 (68) 178 (26) 492 (0.118) 10.4 (6.0) 100 (212) 13.3 (7.4) 172 (25) 508 (0.121) 11.5 (6.6) 200 (392) 14.2 (7.9) 167...
Abstract
View article
PDF
Centralloy HT E is a cast nickel alloy with very good high-temperature properties. This datasheet provides information on composition and tensile properties. It also includes information on casting, machining, and joining. Filing Code: Ni-709. Producer or source: Schmidt & Clemens Inc..