Alloy Digest (2019) 68 (7): SA-849.
Published: 01 July 2019
... CP-K 900Y 1180T is one of a family of omplex-phase steels, CP-W and CP-K, that offer very high strengths and yield points. They are particularly suitable for weight-saving production of cold-formed, crash-relevant automotive components such as side impact intrusion beams, B-pillar reinforcements...