Alloy Digest (1993) 42 (12): Cu-594.
Published: 01 December 1993
... COPPER ALLOY NOS. C14300 AND C14310 are deoxidized coppers with a small percentage of Cd to resist thermal softening. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and...
Journal Articles
Alloy Digest (1986) 35 (6): Cu-511.
Published: 01 June 1986
... composition Copper alloy no. C14300 corrosion-resistant alloys elasticity electrical applications hardness heat treatability joinability machinability physical properties shear strength solderability tensile properties weldability workability UNS C14300 I c amber mm -A I - DATA ON WORLD WIDE...