Alloy Digest (1993) 42 (12): Cu-594.
Published: 01 December 1993
... COPPER ALLOY NOS. C14300 AND C14310 are deoxidized coppers with a small percentage of Cd to resist thermal softening. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining...