Alloy Digest (1973) 22 (9): SS-109.
Published: 01 September 1973
... COOPER Alloy PH-55A comprises three grades each of which offers a different combination of corrosion resistance, high hardness, high strength and machinability. They were developed to meet the combined requirements of high corrosion, abrasion and erosion resistance. They maintain their corrosion...
Journal Articles
Alloy Digest (1961) 10 (5): SS-117.
Published: 01 May 1961
... COOPER PH-55B is a high-strength high-ductility alloy recommended for corrosion resistance of parts subjected to a combination of stress and shock. It responds to an age-hardening heat treatment. This datasheet provides information on composition, hardness, and tensile properties as well...