Alloy Digest (1989) 38 (9): Ti-93.
Published: 01 September 1989
... Commercially pure wrought titanium, Grade 12 is used in the chemical industry where conditions are mildly reducing or varying between oxidizing and reducing. It is immune to formic acid, aerated or non-aerated. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (10): Ti-131.
Published: 01 October 2003
... ASTM B 367 GRADE C-3 is a commercially pure titanium casting alloy. For the most part, titanium casting alloys are based on traditional wrought product compositions. Several data sheets for commercially pure (CP) grades of wrought titanium alloys have been published in Alloy Digest. This data...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (11): Ti-132.
Published: 01 November 2003
... ASTM B 367 GRADE Ti-Pd8A is commercially pure titanium casting alloy with a small palladium addition. For the most part, titanium casting alloys are based on traditional wrought product compositions. The small palladium addition to this grade improves corrosion resistance while not changing any...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (3): Ti-164.
Published: 01 March 2020
... Sandmeyer Titanium Grade 2/2H (UNS R50400) is an unalloyed commercially pure titanium. It is the most widely used commercially pure titanium grade. It offers a combination of moderate strength and good ductility, with outstanding corrosion resistance in many challenging service environments...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (1): Ti-162.
Published: 01 January 2020
... ATI corrosion-resistant commercially pure (CP) titanium represents a family of unalloyed (Grades 1, 2, 3 and 4) and palladium alloyed (Grades 7, 11, 16 and 17) CP titanium that is produced as plate, sheet and strip. It is the material of choice for many corrosive chemical environments, including...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (11): Ti-184.
Published: 01 November 2021
... is galvanically coupled to an active metal or an sourced from M.J. Donachie, Jr., Titanium: A Technical Guide, impressed current or the pH is less than 3 or greater than 12. 2nd ed., ASM International, 2000. Information on corrosion sourced from Corrosion-Resistant Comparable Grades Titanium: Commercially Pure...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (10): Ti-183.
Published: 01 October 2021
... Austral Wright Titanium Grade 2 (UNS R50400) is an unalloyed, commercially pure titanium grade. It is the most widely used commercially pure titanium grade. It offers a combination of moderate strength (similar to that of austenitic stainless steels), good formability, outstanding corrosion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (4): Ti-177.
Published: 01 April 2021
... L. Klein Titan Grade 2 is an unalloyed, commercially pure titanium grade. It is the most widely used commercially pure titanium grade. It offers a combination of moderate strength and good ductility, with outstanding corrosion resistance in many challenging service environments. L. Klein Titan...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (12): Ti-74.
Published: 01 December 1979
... RMI 0.2% Pd is a grade of commercially pure titanium to which up to 0.2% palladium has been added. It has a guaranteed minimum yield strength of 40,000 psi with good ductility and formability. It is recommended for corrosion resistance in the chemical industry and other places where...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (2): Ti-11.
Published: 01 February 1957
... properties tensile properties weldability workability All ov MST GRADE III Filing Code: Ti-11 Titanium FEBRUARY 1957 DIGESTd - DATA ON WORLD WIDE METALS AND ALLOYS Prrbljrbd b Engineering Alloys Dii. IrlC. Upper Monrclair, New Jersey MST GRADE III (Commercially Pure Titanium) MST Grade III...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (8): Ti-72.
Published: 01 August 1979
... RMI 40 is a grade of commercially pure unalloyed titanium. It has a guaranteed minimum yield strength of 40,000 psi with good ductility and formability. Its strength is about the same as that of the annealed austenitic stainless steels. It has good impact properties at low temperatures...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (2): Ti-175.
Published: 01 February 2021
... ATI CP Grade 7 Titanium is an unalloyed titanium grade that contains 0.12–0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 7 Titanium is used in applications requiring excellent corrosion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (9): Ti-182.
Published: 01 September 2021
... ATI CP Grade 16 Titanium is an unalloyed titanium grade that contains 0.04–0.08% Pd. This Pd-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 16 Titanium is used in applications requiring excellent corrosion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (6): Ti-179.
Published: 01 June 2021
... ATI CP Grade 11 Titanium is an unalloyed titanium grade that contains 0.12-0.25% Pd. This palladium-containing alloy extends the range of application of commercially pure (CP) titanium in HCl, H3PO4, and H2SO4 solutions. ATI CP Grade 11 Titanium is used in applications requiring excellent...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (9): Ti-114.
Published: 01 September 1998
... are intermediate strength, heat treatable, alpha/beta titanium alloys possessing excellent fabricability. The alloys are cold formable and easily welded, much like the commercially pure (unalloyed) grades of tita- nium. The alloys offer nearly double the strength at both room and elevated temperatures over TIMETAL...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (11): Ti-122.
Published: 01 November 2001
...) range and finish at 705 760 °C (1300 1400 °F). Most forming operations in sheet stock can be performed at room temperature, but warm forming at 150 425 °C (300 800 °F) will reduce springback and power requirements. TIMETAL-35A is the commercially pure grade having the lowest tensile strength. Sheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (6): Ti-86.
Published: 01 June 2022
... Austral Wright Titanium Grade 7 (UNS R52400) is a corrosion resistant alpha titanium alloy with mechanical properties similar to those of the commercially pure grades. The presence of 0.12–0.25 % palladium in this alloy improves its corrosion resistance, particularly in mineral acids and strong...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (3): Ni-346.
Published: 01 March 1987
... No. NO2230 (Commercially Pure Nickel) UNS No. NO2230 was designed for use in active cathodes. It is essentially free from titanium. Its close!y controlled composition makes it useful for certain special electron-tube applications. Composition: Physical Constants: Range Density, lbicu in. 0.321 Nickel...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (7): Ni-261.
Published: 01 July 1979
... NIMAG 130 is a commercially pure grade of nickel for use in active cathodes. Its composition is controlled closely by vacuum melting so that it may be used in a number of special applications in electron-tube manufacture. The titanium content of Nimag 130 is kept at a low level (nominally 0.003...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (8): Al-134.
Published: 01 August 1979
... ALUMINUM 1060 is a commercially pure grade of aluminum (99.6% minimum aluminum) recommended for applications requiring one or more of the following characteristics: excellent formability, excellent resistance to corrosion and excellent weldability. It has relatively low strength. It is recommended...