Alloy Digest (1969) 18 (9): Cb-16.
Published: 01 September 1969
... COLUMBIUM C-129Y is a columbium-tungsten-hafnium refractory alloy having good high temperature properties along with good heat and oxidation resistance. It is recommended for missiles, space craft and various high temperature applicatios. This datasheet provides information on composition...