Alloy Digest (1974) 23 (6): Ni-205.
Published: 01 June 1974
... COLMONOY No. 62SA comprises a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat and galling. Colmonoy No. 62SA is supplied as atomized powder for application with Wall Colmonoy's SPRAYWELD Process. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1998) 47 (9): Ni-545.
Published: 01 September 1998
... hydroxide, salt water, and sulfuric acid. It also has a low coefficient to friction to reduce metal-to-metal adhesive wear loss. Colmonoy and Fusewelder are registered trademarks, and Fuseweld, Sprayweld, and Spraywelder are trademarks of Wall Colmonoy Corp. The ahoy-is covered under U.S. patent No...