1-20 of 22 Search Results for

COLMONOY No. 5

Sort by
Journal Articles
Alloy Digest (1975) 24 (5): Ni-217.
Published: 01 May 1975
... COLMONOY NO. 5 comprises a chromium-boride-containing, nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat and galling. Deposits, which have only moderate hardness (Rockwell C 45-50), may be machined with carbide tooling. Also, deposits have fairly good...
Journal Articles
Alloy Digest (1977) 26 (3): Ni-242.
Published: 01 March 1977
... Deposits 28-33 Class 6* Class 2* Class 1* Class 5 * Class 3 * Class 3 * Investment Castines 28-33 Class 6* Class 2* Class 1* Class 5 * Class 3* Class 3 * *Classified on a comparative basis of 1 (highest) to 6 (lowest). Table 2 - TYPICAL WHEELS FOR GRINDING COLMONOY No. 22 (Fuseweld and welding rod deposits...
Journal Articles
Alloy Digest (1998) 47 (9): Ni-545.
Published: 01 September 1998
... Colmonoy 98 is a nickel-base alloy with high corrosion resistance, particularly to sodium hydroxide, salt water, and sulfuric acid. It also has a low coefficient to friction to reduce metal-to-metal adhesive wear loss. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2009) 58 (6): Ni-670.
Published: 01 June 2009
... to cracking under impact. A high volume of carbide particles uniformly distributed in the matrix provides excellent abrasion resistance. This alloy is not recommended for applications where the abrasive particles are extremely fine (less than 5 m) or in a slurry form. Producer: Wall Colmonoy Corporation...
Journal Articles
Alloy Digest (2009) 58 (7): W-29.
Published: 01 July 2009
... cracking under impact conditions. A high volume of carbide particles uniformly distributed in the matrix provides excellent abrasion resistance. Colmonoy 80 PTA is not recommended for applications where the abrasive particles are extremely fine (less than 5 m) or in a slurry form. Producer: Wall Colmonoy...
Journal Articles
Alloy Digest (2008) 57 (9): Ni-665.
Published: 01 September 2008
... Colmonoy No. 63HV is a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat, and galling. The hardness of Colmonoy 63HV ranges to 58–61 HRC, and it is resistant to abrasion. Colmonoy 63HV is sized exclusively for high-velocity oxygen-fuel thermal spray systems...
Journal Articles
Alloy Digest (1977) 26 (1): Ni-239.
Published: 01 January 1977
... resistance Class 5 * Red hardness Class 3* Weldability Colmonov No 3 4 .- . Class 3* Colmonoy No. 24 Class 4* *Classified on a comparative scale of 1 (highest) to 6 (Icwest). Table 2 - TYPlCAL WHEELS FOR GRINDING COLMONOY No. 23A AND No. 24 (Fuseweld deposits) Make Surface 0.310 8.60 1950 1790 of Horizontal...
Journal Articles
Alloy Digest (1976) 25 (5): Ni-227.
Published: 01 May 1976
... impact,* ft-lb (Average) 5 *Special specimens having ?&inch-radius notch and polished to remove all possibility of stress concentrations. (Reference: Men1 Progress, May 1959, Impact Testing for Calculating Tool Steels Table 3 - TYPICAL WHEELS FOR GRINDING COLMONOY No. 42SA Surface Make of Horizontal...
Journal Articles
Alloy Digest (1977) 26 (6): Ni-245.
Published: 01 June 1977
... No. 56 is supplied as bare rods (5/32,3/16. l/4,5/16, and 3/8-m diameter) to be applied by oxyacetylene or TIG (Heliarc) welding processes. It is supplied also as crushed powder for application with the Colmonoy Spraywelder or Fusewelder and plasma-spray transferred-arc process. Applications: Colmonoy...
Journal Articles
Alloy Digest (1996) 45 (3): Ni-504.
Published: 01 March 1996
..., medium dressing for finish- ing. DOI: 10.31399/asm.ad.ni0504 Copyright © ASM International® 1996 Table 1 Grinding Wheels for Nickel-Base Colmonoy Alloys Makd Ha verti=w whd SpjldL w Cyrodrpl Iaunlal Ceaalas Todi&om Ahuic sC536IawI SCS36K.5 WI SC5 36L4 VtTl sC536L4vuI bYQ= C-361H8-V32 soA361cn24 C-461X...
Journal Articles
Alloy Digest (1975) 24 (12): Ni-222.
Published: 01 December 1975
... COLMONOY No. 4 is a nickel-base alloy containing chromium boride. It is recommended for hard surfacing parts to resist wear, heat, corrosion and galling. Deposits, which have only moderate hardness (Rockwell C 35-40), can be machined with carbide tooling. Also, deposits have fairly good...
Journal Articles
Alloy Digest (1963) 12 (1): Ni-78.
Published: 01 January 1963
... Colmonoy No. 6 is a high-carbon, nickel-base alloy recommended for hard facing parts to resist wear, corrosion, heat and galling. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1998) 47 (11): Ni-547.
Published: 01 November 1998
... Colmonoy 730 is a tough Ni-Cr-W matrix alloy that holds extremely hard tungsten-carbide particles with a finer mesh tungsten carbide than Colmonoy 750 (Alloy Digest Ni-546, October 1998). The alloy is used on pump plungers and sleeves for protection from fine-particulate abrasive conditions...
Journal Articles
Alloy Digest (1995) 44 (11): Ni-489.
Published: 01 November 1995
... COLMONOY No. 69SC is a nickel-base hard surfacing alloy incorporating the qualities of Colmonoy No. 69 (Alloy Digest Ni-206, July 1974) with other enhancements. Its extended plastic range means that sagging and running of other-than-horizontal surfaces during finishing is virtually eliminated...
Journal Articles
Alloy Digest (1976) 25 (10): Co-74.
Published: 01 October 1976
... WALLEX No. 40 is a self-fluxing, cobalt-base hard-surfacing alloy with excellent resistance to a combination of corrosion and abrasion and relatively good impact properties. It has excellent red hardness and weldability. It is supplied only as atomized powder for application with Wall Colmonoy's...
Journal Articles
Alloy Digest (1964) 13 (1): Co-36.
Published: 01 January 1964
... toughness, and deformation. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Co-36. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM...
Journal Articles
Alloy Digest (2003) 52 (9): Ni-614.
Published: 01 September 2003
... Nicrobraz 31 is a high-chromium, oxidation-resistant nickel braze filler metal with enhanced flow properties. This datasheet provides information on composition. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-614. Producer or source: Wall Colmonoy...
Journal Articles
Alloy Digest (2009) 58 (10): Ni-674.
Published: 01 October 2009
..., and powder metal forms. Filing Code: Ni-674. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 2009 2009 ASM International chemical composition corrosion-resistant alloys joinability nickel brazing filler metals...
Journal Articles
Alloy Digest (1994) 43 (7): Ni-457.
Published: 01 July 1994
..., physical properties, and hardness. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-457. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 1996 1996 ASM International chemical...
Journal Articles
Alloy Digest (1994) 43 (3): Cu-597.
Published: 01 March 1994
.... Filing Code: CU-597. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition copper brazing filler metals copper powder CuBraz FILLER METAL joinability physical...