Journal Articles
Alloy Digest (1975) 24 (12): Ni-222.
Published: 01 December 1975
... COLMONOY No. 4 is a nickel-base alloy containing chromium boride. It is recommended for hard surfacing parts to resist wear, heat, corrosion and galling. Deposits, which have only moderate hardness (Rockwell C 35-40), can be machined with carbide tooling. Also, deposits have fairly good...
Journal Articles
Alloy Digest (2002) 51 (1): SS-843.
Published: 01 January 2002
... 1 for the recommended current ranges for the two Colmonoy alloys. When overlaying surfaces that have been worn down more than 6.35 9.53 mm (1/4 3/8 in the worn areas should first be built up with a lower-cost weld metal. While Colmonoy No. 1 and Special No. 1 have sufficient ductility to provide...
Journal Articles
Alloy Digest (1977) 26 (1): Ni-239.
Published: 01 January 1977
... resistance Class 5 * Red hardness Class 3* Weldability Colmonov No 3 4 .- . Class 3* Colmonoy No. 24 Class 4* *Classified on a comparative scale of 1 (highest) to 6 (Icwest). Table 2 - TYPlCAL WHEELS FOR GRINDING COLMONOY No. 23A AND No. 24 (Fuseweld deposits) Make Surface 0.310 8.60 1950 1790 of Horizontal...
Journal Articles
Alloy Digest (1995) 44 (12): Ni-493.
Published: 01 December 1995
... of media. Cohonoy No. 83 is especially well suited for application to SAE 4 140 and 4130 alloy steel, as well as to 400 series Figure 1 - Photomicrograph of Colmonoy 83 deposit (150x). WARNING: Welding may produce fumss and gases hazardous to health. Avoid breathing these fumes and gases. Use adequate...
Journal Articles
Alloy Digest (1996) 45 (3): Ni-504.
Published: 01 March 1996
... joinability machinability oxidation resistance physical properties powder metal products thermal properties I Filing Code: Ni-504 A a1 m Nickel Alloy COLMONOY@ NCI. 21 1 c t a- March 1996 -u DATA ON WORLD WIDE METALS AND ALLOYS - D/GE3 CCopy+@w 1996, AS.4 Inremarkmal. AU nghrs...
Journal Articles
Alloy Digest (2008) 57 (9): Ni-665.
Published: 01 September 2008
... tooling. See Table 3 for recommendations on grinding wheels. Table 2 JP 5000 parameters for spraying Colmonoy 63HV Gun barrel, mm (in.) 100 (4) Spray distance, mm (in.) 355 (14) Coating thickness, mm (in.) >1.52 (>0.060) Spray rate, kg/h (lb/h) 4.5 5.4 (10 12) Water temperature, °C (°F) Incoming 20 (70...
Journal Articles
Alloy Digest (1963) 12 (1): Ni-78.
Published: 01 January 1963
.../4 rod use 180-2 10 amps. Workobi lity: This alloy cannot be forged. (see Welding above; Colmonoy No. 6 may be hot formed while in tie plastic scare) Specification Equivalents: AMS 4775A Brazing Alloy (Rod) ASTM A399-56T, Types RNiCr-C & ENiCr-C, Surfacing Welding Rod and Electrode AWS A5.13-561...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-429.
Published: 01 May 1993
... COLMONOY NO. 88 is a nickel-based hard-surfacing alloy with bimetallic carbides for maximum wear resistance. This datasheet provides information on composition, physical properties, and hardness. It also includes information on machining and powder metal forms. Filing Code: Ni-429. Producer...
Journal Articles
Alloy Digest (1995) 44 (11): Ni-489.
Published: 01 November 1995
... COLMONOY No. 69SC is a nickel-base hard surfacing alloy incorporating the qualities of Colmonoy No. 69 (Alloy Digest Ni-206, July 1974) with other enhancements. Its extended plastic range means that sagging and running of other-than-horizontal surfaces during finishing is virtually eliminated...
Journal Articles
Alloy Digest (1994) 43 (12): Ni-472.
Published: 01 December 1994
...-472. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys ductility hardness joinability machinability NICROBRAZ 160 physical...
Journal Articles
Alloy Digest (1994) 43 (3): Cu-597.
Published: 01 March 1994
.... Filing Code: CU-597. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition copper brazing filler metals copper powder CuBraz FILLER METAL joinability physical...
Journal Articles
Alloy Digest (1995) 44 (1): Ni-476.
Published: 01 January 1995
... resistance as well as joining. Filing Code: Ni-476. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys hardness joinability NICROBRAZ 170...
Journal Articles
Alloy Digest (1994) 43 (7): Ni-457.
Published: 01 July 1994
... Forms Available: -140 mesh atomized powder. (Mix with Nicrobraz Ce- ment or Cement S to apply), powder in suspension for use in applicator, plastic bonded sheet, transfer tape, and flux-powder paste and cast rod. Producer: Wall Colmonoy Corp. Madison Heights, Ml 48071-1650 USA (313) 5856400 Ni-4.!57% ...
Journal Articles
Alloy Digest (1994) 43 (8): Ni-460.
Published: 01 August 1994
.... Filing Code: Ni-460. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys hardness honeycomb structures joinability nickel brazing filler...
Journal Articles
Alloy Digest (1964) 13 (1): Co-36.
Published: 01 January 1964
... toughness, and deformation. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Co-36. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM...
Journal Articles
Alloy Digest (1997) 46 (4): Ni-525.
Published: 01 April 1997
... information on corrosion resistance as well as joining. Filing Code: Ni-525. Producer or source: Wall Colmonoy Corporation. Producer or Source: Wall Colmonoy Corporation Copyright © ASM International® 1997 1997 ASM International chemical composition corrosion-resistant alloys hardness...
Journal Articles
Alloy Digest (1992) 41 (8): SS-533.
Published: 01 August 1992
... tests. Table 4 -TYPICAL ANNEALED PLATE PROPERTIES 1900 OF Anneal Temperature U-l-S Gage ksi (MM -- 7/8 124 (855) @-lOOOF - 2 120 (827) 0.2% YS Elong. Hardness CVN ksi WW % in 2 Rockwell (Ft-lbs) 50 (345) 50 B92 217 125 52 (358) 54 DOI: 10.31399/asm.ad.ss0533 Copyright © ASM International® 1996 Table...