Skip Nav Destination
Close Modal
Search Results for
COLMONOY No. 22
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-5 of 5 Search Results for
COLMONOY No. 22
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (3): Ni-242.
Published: 01 March 1977
...-iron repair are Colmonoy No. 20 (oxyacetylene rod), and Colmonoy Nos. 21, 23A and 24 (Fuseweld Powders). Of all these, Colmonoy No. 22 would be chosen for easiest application (flowability) and finishing, in situations calling for larger areas of repair. A deposit of Colmonoy No. 22 has high oxidation...
Abstract
View article
PDF
COLMONOY No. 22 is a nickel-base alloy supplied as atomized powder, welding rod and investment castings. The powder is applied with Colmonoy's FUSEWELD process to repair cast-iron parts. The investment castings are used in the glass industry as forming tools (plungers, baffles and sleeves) and as welding rod for repairing cast-iron glass-container molds and components. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion and wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: Ni-242. Producer or source: Wall Colmonoy Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (9): Ni-545.
Published: 01 September 1998
...-surfacing alloys. 411 test coupons were encapsulated by spray-and-fuse methods and totally immersed in media at 22 C (72 F) for 72 h. un- less otherwise noted. See Table 2. Tests show that Colmonoy 98 is particularly corrosion resis- tant to sodium hydroxide. deionized water. salt water. and sul- furic...
Abstract
View article
PDF
Colmonoy 98 is a nickel-base alloy with high corrosion resistance, particularly to sodium hydroxide, salt water, and sulfuric acid. It also has a low coefficient to friction to reduce metal-to-metal adhesive wear loss. This datasheet provides information on composition, physical properties, microstructure, and hardness. It also includes information on corrosion and wear resistance as well as machining, joining, and powder metal forms. Filing Code: Ni-545. Producer or source: Wall Colmonoy Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (4): Ni-689.
Published: 01 April 2011
... DELORO 15, 21, 22, and 25 are prealloyed, gas-atomized, nickel-base powders for repair of glass-forming molds. This datasheet provides information on composition, physical properties, and hardness. It also includes information on powder metal forms. Filing Code: Ni-689. Producer or source...
Abstract
View article
PDF
DELORO 15, 21, 22, and 25 are prealloyed, gas-atomized, nickel-base powders for repair of glass-forming molds. This datasheet provides information on composition, physical properties, and hardness. It also includes information on powder metal forms. Filing Code: Ni-689. Producer or source: Stellite Coatings.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (9): Ni-614.
Published: 01 September 2003
... Nicrobraz 31 is a high-chromium, oxidation-resistant nickel braze filler metal with enhanced flow properties. This datasheet provides information on composition. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-614. Producer or source: Wall Colmonoy...
Abstract
View article
PDF
Nicrobraz 31 is a high-chromium, oxidation-resistant nickel braze filler metal with enhanced flow properties. This datasheet provides information on composition. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-614. Producer or source: Wall Colmonoy Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (8): SS-533.
Published: 01 August 1992
... 7.862 See Table 1 28.1 x 106 193 x 10 1.011 1.011 1.014 1.015 Table 1 - COEFFICIENT OF THERMAL EXPANSION, LINEAR F ( C) AL/L/ Fx@ AL/L/T x lOA 72-200 (22-93) 8.98 16.2 72400 (22-204) 8.96 16.1 72-600 (22-3 16) 9.60 17.3 72-800 (22427) 10.19 18.3 72-1000 (22-538) 10.46 18.8 Table 3 - EFFECT OF COLD...
Abstract
View article
PDF
NITRONIC 30 is a nitrogen-strengthened stainless steel with a good combination of strength, corrosion and wet abrasive wear resistance and economy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, and deformation. It also includes information on corrosion and wear resistance as well as forming, heat treating, and joining. Filing Code: SS-533. Producer or source: Armco Advanced Materials Corporation.