Alloy Digest (2008) 57 (7): Ni-664.
Published: 01 July 2008
... Colmonoy No. 43HV comprises a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat, and galling. Deposits that have moderate hardness have increased ductility and slightly less resistance to abrasion than Colmonoy 53HV. Deposits can be finished by grinding or...